Last Updated: December 20, 2021
Study on Different Laboratory Equipments of a Modern Dye House
Rofiquzzaman Raju
Chittagong Textile Engineering College
Contact: 01714419781
Email: [email protected]
Introduction:
Satisfaction of customer demands is the quality of a product. It is the extent of excellence of a product that indicates that whether it meets the customer ultimate demand or not. As textiles, an integrated word is related to different segments and each segment is responsible to meet up the requirements of subsequent segments and finally the ultimate user. Dyeing, the process of coloring textile materials with some medium. It is the section in which raw fabrics are dyed with coloring materials i.e. dyes in some medium i.e. water along with several chemicals. Fabrics are colored as per the buyer requirements. Before going to the bulk production, a sample fabric is dyed in the dyeing lab. If the desired shade is produced here then it is go for bulk production at large amount. However, primary recipe to develop particular shade is prepared here and then finally implemented in the production section. A standard quality lab provides all opportunities to produce particular shade without any disturbance. Besides, the different tests are done in the physical lab to evaluate the different parameters of dyed fabric. Tests conducted in the physical lab basically based on the buyer requirements. During testing, different types of testing method are followed which is varied from buyer to buyer. To learn this, an observation was done at ECHO-TEX LIMITED; an export-oriented apparel industry produces all types of knitting garments. In this article, discussion will be done on dyeing lab of that factory.
Objects:
- To know the different chemicals and equipments used in the modern dye house.
- To understand about the different test carried out in the physical lab.
- To know the responsibility of different managerial designation in the modern dye house.
- Understanding the function of different equipments used in dye house.
Factory Agenda:
- Name of the Project: ECHOTEX LTD.
- Location: Chandra pallibidyut, Kaliakoir, Gazipur.
- Established year: 2003
- Status:100% Export Oriented Knit composite
- Project cost: TK. 2500 crore
- Production capacity: 2100000 pcs/month
- Man power: 7000 people
Layout of the Dyeing lab:

Management structure and their responsibility of the dyeing lab:

Types of Dyeing lab:

Name of the Machine Used in Chemical Lab:
Machine No.01 and 02
Specification of the machine:
- Name: Sample dyeing machine
- Brand Name: Data color AHIBA IRTM
- Origin: U S A
- No. of pot: 19
- Heating system: Infrared
- Sample wt. =5gm

Function: To dye lab dip based on buyer requirements.
Machine No. 03:
Specification of the machine:
- Name: Sample dyeing machine
- Brand Name: Mathis LABOMAT
- Origin: Switzerland
- No. of pot: 23
- Heating system: Infrared
- Sample wt. =10gm

Function: To dye lab dip.
Machine No.04
Specification of the machine:
- Name: Rotawash Color Fastness Tester
- Brand: SDL International
- Model: M228
- Origin: England
- No. of pot: 8

Function: Treating the fabric sample with water to determine color fastness to washing.
Machine No.05
Specification of the machine:
- Name: Sun test CPS+ machine
- Brand: SDL International
- Origin: England
- Lamp capacity=500W

Function: Exposing the fabric sample to determine color fastness to light.
Machine No.06
Specification of the machine:
- Name: Oven dryer machine
- Specification:
- Brand: XIEMAN Rapid
- Origin: China

Function: To dry fabric sample at required sample.
Machine No.07
Specification of the machine:
- Name: Washing machine
- Brand: SIEMENS
- Origin: Germany
- Capacity: 5.5 kg
- Speed: 1000rpm

Function: To wash the fabric sample at particular temperature.
Machine No.08
- Specification of the machine:
- Name: Quick wash plus machine:
- Specification:
- Brand: SDLATLAS
- Origin: UK

Function: To wash the fabric sample very quick manner with respect to normal washing.
Machine No.09
Specification of the machine
- Name: Shaker machine
- Specification:
- Brand: Rapid
- Origin: China

Function: After dyeing soaping is done by this machine.
Machine No.10
Specification of the machine:
- Name: Robolab machine

Function: To prepare dye solution based on recipe amount for dyeing.
Machine No.11
Specification of the machine:
- Name: Spectrophotometer machine
- Model: 650
- Origin: USA

Function:
- Recipe develops from standard sample
- Check CMC value of Sample to evaluate it.
Name of the Machine used in Physical Lab: –
Tests done in Physical lab are:
- Dimensional stability.
- Shrinkage
- Spirality
- Angular spacing
- Pilling test
- Rubbing Test
- GSM
- Color fastness to light
- Color fastness to water
- Color fastness to washing
- Color fastness to perspiration (Acid & Alkali Solution)
- Color fastness to SALIVA
- Color fastness Phenolic Uline
Machine No.01
Specification of the machine:
- Name: Pilling tester
- Brand: SDL ATLAS
- Origin: UK

Function: Treating the fabric sample to create pile on the sample fabric surface.
Testing parameters:
- Sample size: (12.5 x 12.5) cm, Method: ISO 12945-1:2001
- Tube size: (14 x 2.6) cm, Revolution: 14400
- Speed: 60 rpm, Test sample: 4 pcs
- Course wise: 2 pcs and Wales wise: 2 pcs
Machine No.02
Specification of the machine:
Name: Crockmeter
Test parameters:
- Sample size: Dyed fabric – (14 x5) cm
- White Test Cloth – 5 cm ´ 5 cm
- Method: ISO 105x2L: 2002
- Revolution: 10cycle/10sec
- Weight: 9N

Function: Rubbing the fabric sample to measure color fastness properties.
Machine No.03
Specification of the machine:
- Name: Overlock sewing machine
- Brand: Juki
- Origin: Japan

Function: To sew the fabric for dimensional stability measurement test.
Measurement of Dimensional stability:
Dimensional stability:
This is the test by which dimensional stability of fabric (i.e.: shrinkage & spirality) are measured. For this test, fabric has to be washed per care label code.
Test specimen & Equipment:
- Sample size: outside = (50×50) cm and Inside = (35×35) cm
- Method: ISO 6330: 2001 2A/5A
- Equipment used: washing machine (Rota wash)
- Washing at 400C X 41’, As per care label code.
Procedure:
- Conditioning: Put the sample in table for 4 hrs. for conditioning before starting test.
- Cut the sample 50×50 cm & benchmark should be 35×35 cm.
- Stitch the sample (3 sides) by over lock sewing machine.
- Put sample in washing machine and run according to buyer’s choice.
Shrinkage calculation:
……………………………………………………..31.5 + 31 + 30.8
After test: Inside measurement= ………………………………… = 31.1cm
……………………………………………………………….3
……………………………Before wash – After wash
Shrinkage = …………………………………………………….. x 100%
……………………………………..Before wash
……….35 – 31.5
= ………………………… x 100 =11.14 %
……………35

Spirality Calculation:

Total distance = 47 cm.
Average spiral distance = (2+3)/2 = 2.5 cm
……………………Average spiral distance
Spirality = ……………………………………………. x 100% = (2.5×100)/47 = 5.32 %
………………………….Total distance
Conclusion:
The equipments of dye house are varied from factory to factory. The ECHOTEX LTD dye house is well equipped with different equipments along with necessary chemicals by which various types of lab dip can be developed and a number of tests are done in the physical lab with assured quality. All the equipment’s are sufficiently enough to meet the buyer requirements successfully. But all the tests cannot be conducted here.
You may also like:
- List of Physical Testing Machines in Dyeing Lab
- List of Chemical Testing Equipments for Dyeing Lab
- Different Types of Testing Equipments Used in Textile Lab
- Spinning Testing Lab Equipments, Their Specifications and Functions
- Different Types of Testing and Approval Required for Fabric to Garment Manufacturing Process
Founder & Editor of Textile Learner. He is a Textile Consultant, Blogger & Entrepreneur. Mr. Kiron is working as a textile consultant in several local and international companies. He is also a contributor to Wikipedia.