MCQ Questions and Answers on Textiles and Clothing
Jahanara Akter
Fashion Designer & Ex-Lecturer,
Dept. of Fashion Design
KCC Women’s College (Affiliated by Khulna University)
Khulna, Bangladesh
This article is written for textile engineering and fashion design students, teachers and professionals. Specially this article will be helpful for job seekers and students who are preparing for viva board. MCQ questions and answers focus on fiber, spinning, weaving, knitting, washing, testing and quality control, apparel inspection, fashion designing etc. In this article 1000 Multiple Choice Questions (MCQ) are listed with answers key.

1000 Multiple Choice Questions (MCQ) and Answers on Textiles and Clothing
1) The short length man-made yarns are called ___________ yarns. (Answer = C)
A. Complex B. Filament
C. Spun D. None of these
2) Which is an elastomeric fiber? (Answer = D)
A. Acrylic B. Mod Acrylic
C. Nylon D. Spandex
3) Spinning of yarn means_________ . (Answer = B)
A. Denier B. Twisting
C. Tex D. Pulling
4) Symmetrical balance occurs when the space within a garment is divided into _________ parts. (Answer = A)
A. Equal B. Un equal
C. Three D. Four
5) When the design elements work well together _______ is achieved. (Answer = D)
A. Rhythm B. Balance
C. Proportion D. Harmony
6) Triangular-shaped folds of fabric stitched to control fullness are called __________. (Answer = C)
A. Gathers B. Pleats
C. Darts D. Hem
7) The process of converting waste material into new product and objects is called __________. (Answer = D)
A. Recreation B. Redesigning
C. Reformation D. Recycling
8) The process of converting fibers directly into fabric is __________. (Answer = D)
A. Weaving B. Spinning
C. Knitting D. Felting
9) Colors which are exact opposite to each other on color wheel are _________. (Answer = C)
A. Analogous B. Monochromatic
C. Complimentary D. Tetrade
10) Lightness or darkness of a color is known as ____________. (Answer = A)
A. Value B. Intensity
C. Brightness D. Dullness
11) There are ___________ neutral colors. (Answer = C)
A. 1 B. 4
C. 3 D. 5
12) Flax is a __________ fiber. (Answer = A)
A. Cellulosic B. Proteinic
C. Synthetic D. Man Made
13) __________ is the art of creating designs for knitted, woven and non-woven fabrics. (Answer = B)
A. Illustrations B. Textile Designs
C. Paintings D. Sketches
14) _________French term for exclusive one-of-kind” high fashion”. (Answer = D)
A. Boutique B. Show room
C. Out let D. Haute couture’s
15) _______________ is the basic unit of textile. (Answer = C)
A. Fabric B. Yarn
C. Fiber D. Cloth
16) Solution dyeing is mostly used for ________ fibers. (Answer = C)
A. Wool B. Natural
C. Synthetic D. Cellulosic
17) Creativity in textile is also known as ___________. (Answer = D)
A. Fabric B. Clothing
C. Textiles D. Designing
18) ___________ designing shows awkward look in clothing. (Answer = B)
A. Good B. Incomplete
C. Unstitched D. Raw
19) ______________ designers sell their designs to fashion houses. (Answer = B)
A. Full-time B. Freelance
C. Self employed D. In-house
20) Grey cloth is also known as _________. (Answer = D)
A. Toile B. Kutch
C. Maison D. Unfinished fabric
21) First synthetic dye was developed in ________. (Answer = A)
A. 1856 B. 1857
C. 1858 D. 1859
22) _________ are made specifically for an individual. (Answer = A)
A. Haute-Couture B. Pret wear
C. Special cloths D. Costumes
23) Feel or hand of the fabric is its __________. (Answer = A)
A. Texture B. Strength
C. Fall D. Drape
24) Compounds that color textile is known as __________. (Answer = D)
A. Finished B. Dyes
C. Bleaching D. None of these
25) Which fiber is popularly called ‘Golden fiber’. (Answer = C)
A. Cotton B. Silk
C. Jute D. Flax
26) _________ are forms of art that are created by using your hands. (Answer = C)
A. Hand works B. Designs
C. Handicrafts D. Drawings
27) _________ is an ironing process that adds sheen to the fabric. (Answer = C)
A. Shearing B. Weighting
C. Calendaring D. Embossing
28) The companies that apply only finishes on textiles are…. (Answer = B)
A. Finish Product Supplier B. Converters and jobbers
C. Retail Distributor D. None of These
29) Blends are combination of ……………….. fibers. (Answer = C)
A. Same B. Bonded
C. Different D. None of these
30) The lengthwise yarn in a woven fabric is known as __________. (Answer = C)
A. Selvedge B. Grain
C. Warp D. Weft
31) In a knit, the lengthwise rows of stitches are called __________. (Answer = B)
A. Courses B. Wales
C. Warps D. None of these
32) Bleaching is a ________________ treatment. (Answer = A)
A. Whitening B. Mercerizing
C. Dyeing D. None of these
33) Sizing is a ____________ treatment. (Answer = B)
A. Cleaning B. Finishing
C. Dyeing D. Printing
34) Principles of design are…………. (Answer = D)
A. Proportion B. Balance
C. Rhythm D. All of these
35) The designer of ………………… designed garments for High class. (Answer = B)
A. Haute Couture B. Local
C. Pret D. Both a & b
36) Other name for screen printing is __________. (Answer = D)
A. Digital printing B. Transfer printing
C. Synthetic printing D. Silk screen printing
37) In……………… a mesh is used to transfer ink onto a substrate. (Answer = C)
A. Dyeing B. Batik
C. Screen printing D. Weaving
38) Knitting needles by hand should be __________ inches long. (Answer = A)
A. 7 to 14 B. 1 to 7
C. 14 to 21 D. None of these
39) Color is also known as………………. (Answer = D)
A. Pill B. Dust
C. Paint D. Hue
40) Which one is the protein fiber among the below mentioned fibers? (Answer = D)
A. Cotton B. Jute
C. Rayon D. Silk
41) Which lines add softness and roundness to a garment? (Answer = A)
A. Curved B. Diagonal
C. Vertical D. Horizontal
42) The less expensive copies of designer’s garments are called ___________. (Answer = A)
A. Knock-off B. Seconds
C. B-Grade D. Both a & b
43) If no water penetrate in fabric, it will be__________. (Answer = A)
A. Waterproof B. Water-repellent
C. Stain D. None of these
44) When already dyed fabric is printed, it is called __________. (Answer = C)
A. Double printing B. Another printing
C. Over printing D. All of these
45) Batik is ____ dyeing technique. (Answer = A)
A. Resist B. Tie & Dye
C. Egyptian D. Stock
46) In lab test which fiber dissolved in acetone is? (Answer = B)
A. Nylon B. Acetate
C. Rayon D. Orlon
47) Acetate has only________ sunlight resistance. (Answer = C)
A. Excellent B. Good
C. Fair D. Bad
48) Any style that is accepted for a short period of time called __________. (Answer = C)
A. Tradition B. Classic
C. Fad D. Old-fashioned
49) Surface ornamentation of fabric is called. (Answer = B)
A. Fashion designing B. Textile designing
C. Designing D. None of these
50) __________ are short fibers that measured in inches or centimeters. (Answer = B)
A. Filament B. Staple
C. Coarse D. Bonded
51) Cotton is known as our …………….. crop. (Answer = C)
A. Finished B. Bleached
C. Cash D. Calendered
52) Part of the garment that turns back below the collar is called ______. (Answer = C)
A. Yoke B. Hem
C. Lapel D. Trim
53) Dacron is a trade name of which fiber? (Answer = B)
A. Nylon B. Polyester
C. Spandex D. Acrylic
54) Fabric is treated with heat, moisture and pressure to wool fiber. (Answer = A)
A. Lustering B. Felting
C. Beetling D. Glazing
55) The cohesiveness is the ability of fiber to ___________together. (Answer =B)
A. Elasticity B. Cling
C. Stretch D. Press
56) In which device the finished fabric holds under tension. (Answer = A)
A. Cloth beam B. Shuttle
C. Warp beam D. None of these
57) The ability of fabric to draw moisture away from your body is…. (Answer = A)
A. Wicking B. Absorbency
C. Resiliency D. None of these
58) When dye is applied in specific pattern on fabric is called _______ (Answer = D)
A. Double printing B. Another printing
C. Dyeing D. Printing
59) A fitted section at the shoulders or hips to which the garment is attatched is…. (Answer =B)
A. Collar B. Yoke
C. Hem D. Both A&B
60) Sueding is a _________ treatment. (Answer = B)
A. Cleaning B. Finishing
C. Dyeing D. Printing
61) A clothing review is __________. (Answer = B)
A. Whitening B. Wardrobe plan
C. Cleaning D. Schrenerizing
62) The direction of threads in a woven fabric is known as_________ . (Answer = B)
A. Selvedge B. Grain
C. Warp D. Weft
63) Singeing of cotton is carried out to_________ . (Answer = A)
A. Remove protruding fibers from fabrics surface B. Impart luster
C. Cut long threads from fabrics surface D. Increased pliability of fibers
64) Fabric cut at 45o angle is ________. (Answer = D)
A. Seam allowance B. Seam finish
C. Seam D. Bias
65) _________ is man-made cellulosic fiber. (Answer = A)
A. Rayon B. Acrylic
C. Orlon D. Nylon
66) Country sent dolls dressed in latest fashion to other nations was_________ . (Answer = D)
A. England B. China
C. New york D. France
67) Ancient Egyptians used fiber for bandages for mummification was_________ . (Answer = B)
A. Cotton B. Linen
C. Jute D. Silk
68) Road very important for exchange of luxury textiles between East and West was_________ . (Answer = B)
A. G.T Road B. Silk Road
C. Persia Road D. None of these
69) A-Symmetrical balance occurs when the space within a garment is divided into ___________ parts. (Answer = B)
A. Equal B. Un equal
C. Three D. Four
70) When the design_______ work well together Harmony is achieved. (Answer = D)
A. Figures B. Balance
C. Proportion D. Elements
71) Triangular-shaped folds of fabric stitched to control ________ are called darts. (Answer = C)
A. Gathers B. Pleats
C. Fullness D. Hem
72) The main constituent of wool fiber is __________. (Answer = D)
A. Cellulose B. Casien
C. Reformation D. Keratin
73) This is a yarn producing machine. (Answer = A)
A. Ring-frame B. Spinning
C. Knitting D. Felting
74) Colours which are exact _________ to each other on colour wheel are compliments. (Answer = C)
A. Parallel B. Monochromatic
C. Opposite D. Tetrade
75) Green and blues are _________colors. (Answer = A)
A. Cool B. Intensity
C. Bright D. Dull
76) There are ___________ neutral colors. (Answer = C)
A. 1 B. 4
C. 3 D. 5
77) Flax is a __________ fiber. (Answer = A)
A. Cellulosic B. Protein
C. Synthetic D. Man Made
78) Fashion magazines help in spreading__________ . (Answer = A)
A. Fashion B. Textile Designs
C. Paintings D. News
79) Which of the following is leaf fiber? (Answer = B)
A. Cotton B. Banana
C. Flax D. Sisal
80) Polyester fiber manufactured by_________ spinning method. (Answer = C)
A. Dry B. Wet
C. Melt D. Ring
81) Solution dyeing is mostly used for ________ fibers. (Answer = C)
A. Wool B. Natural
C. Synthetic D. Cellulosic
82) ________ are items worn on the body. (Answer = B)
A. Fabric B. Clothing
C. Textiles D. Designs
83) Points create lines and lines create__________. (Answer = A)
A. Shapes B. Colors
C. Space D. Emotions
84) Which one is strongest weave? (Answer = C)
A. Plain B. Basket
C. Twill D. Satin
85) Muslin is a cotton fabric of _________weave. (Answer = A)
A. Plain B. Twill
C. Maison D. Satin
86) Queen Marie Antoinette started a __________ revolution in France. (Answer = C)
A. Freedom B. 1857
C. Fashion D. Style
87) ___________ are made specifically for an individual. (Answer = A)
A. Haute-Couture B. Pret wear
C. Special cloths D. Costumes
88) _________ is the ability of a fabric to fall under its own weight into wavy folds of different nature. (Answer = D)
A. Texture B. Feel
C. Fall D. Drape
89) Compounds that color textile is known as __________. (Answer = D)
A. Finished B. Dyes
C. Bleaching D. None of these
90) Which fiber is successfully produced in Bangladesh? (Answer = C)
A. Kapok B. Silk
C. Jute D. Flax
91) Hooks, eyes, snaps, buttons and zipper are ______for garments. (Answer = C)
A. Markings B. Designs
C. Fastener D. Facing
92) Buttonholes are of _______ types. (Answer = B)
A. One B. Two
C. Four D. Five
93) The companies that provide raw materials for Fashion Pipeline are called __________. (Answer = B)
A. Finish Product Supplier B. Component Supplier
C. Retail Distributor D. None of These
94) It fits closed to the neck without binding or gapping. (Answer = C)
A. Composite B. Seam
C. Collar or neckline D. None of these
95) Any good fitting of a garment must have the considerable amount of_________. (Answer = C)
A. Selvedge B. Grain
C. Ease D. Looseness
96) Comfort, Appearance, and Durability are the important factors for __________ of the garment. (Answer = C)
A. Color B. Wear
C. Good fitting D. None of these
97) Caustic soda is used in ___________ process. (Answer = B)
A. Whitening B. Mercerization
C. Cleaning D. None of these
98) Fulling is a ____________ treatment. (Answer = B)
A. Cleaning B. Finishing
C. Dyeing D. Printing
99) Color is _____________ of design. (Answer = B)
A. Proportion B. Element
C. Rhythm D. All of these
100) The designer of Haute Couture show a new collection _________ a year. (Answer = B)
A. Once B. Twice
C. Thrice D. Both a & b
101) Other name for screen printing is ___________. (Answer = D)
A. Digital printing B. Transfer printing
C. Synthetic printing D. Silk screen printing
102) In screen printing a ___________ is used to transfer ink onto a substrate. (Answer = C)
A. Net B. Plastic
C. Mesh D. Wood
103) Knitting needles by hand should be ___________ inches long. (Answer = A)
A. 7 to 14 B. 1 to 7
C. 14 to 21 D. None of these
104) Other name for color is ___________. (Answer = D)
A. Pigment B. Dye
C. Paint D. Hue
105) __________ is the oldest type of printing. (Answer = B)
A. Screen printing B. Block printing
C. Transfer printing D. Digital printing
106) Thread count found in type writer ribbon fabric is: (Answer = C)
A. 250 B. 300
C. 350 D. 400
107) Process introduced into the spinning of finer and high quality yarns for cotton is: (Answer = B)
A. Carding B. Combing
C. Slashing D. Roving
108) Dyeing at fiber stage is known as ___________. (Answer = C)
A. Solution dyeing B. Top dyeing
C. Stock dyeing D. None of these
109) When already dyed fabric is printed, it is called ____________. (Answer = C)
A. Double printing B. Another printing
C. Over printing D. All of these
110) Acetate is derived from__________. (Answer = A)
A. Cellulose B. Protein
C. Latex D. Rubber
111) Block printing first originate in ________. (Answer = B)
A. Indonesia B. China
C. Egypt D. Asia
112) Garment cutting and manufacturing is based on __________. (Answer = A)
A. Measurement B. Fit
C. Style D. Fullness
113) Fashion stay for short time period is __________. (Answer = C)
A. Tradition B. Classic
C. Fad D. Old-fashioned
114) Surface ornamentation of fabric is called________ . (Answer = B)
A. Fashion designing B. Textile designing
C. Designing D. None of these
115) __________ are short fibers that measured in inches or centimeters. (Answer = B)
A. Filament B. Staple
C. Coarse D. Bonded
116) Cotton can also be ___________ to give the fiber added strength and luster. (Answer = C)
A. Finished B. Bleached
C. Mercerized D. Calendered
117) Which is an elastomeric fiber? (Answer = D)
D A. Acrylic B. Mod Acrylic
C. Nylon D. Spandex
118) Dacron is a trade name of which fiber? (Answer = B)
A. Nylon B. Polyester
C. Spandex D. Acrylic
119) Fabric is treated with heat and pressure to add luster. (Answer = A)
A. Lustering B. Felting
C. Beetling D. Glazing
120) The ability of fiber to stretch and return to shape is__________. (Answer = A)
A. Elasticity B. Crimp
C. Stretch D. Pliablity
121) In which device the finished fabric holds under tension. (Answer = A)
A. Cloth beam B. Shuttle
C. Warp beam D. None of these
122) The ability of fiber to return to its original shape after stretching is _________ . (Answer = C)
A. Wicking B. Absorbency
C. Resiliency D. None of these
123) When already dyed fabric is printed, it is called… (Answer = C)
A. Double printing B. Another printing
C. Over printing D. Printing
124) The designer of Haute Couture show a new collection _________ a year. (Answer = B)
A. Once B. Twice
C. Thrice D. Both A & B
125) Grass bleaching is applicable for __________ fabrics. (Answer = B)
A. Suede B. Linen
C. Denim D. Printed
126) Bleaching is a ____________ treatment. (Answer = A)
A. Whitening B. Mercerizing
C. Cleaning D. Schrenerizing
127) The direction of threads in a woven fabric is known as__________. (Answer = B)
A. Selvedge B. Grain
C. Warp D. Weft
128) Singeing of cotton is carried out to___________ . (Answer = A)
A. Remove protruding fibers from fabrics surface B. Impart luster
C. Cut long threads from fabrics surface D. Increased pliability of fibers
129) Spinning of yarn means ____________. (Answer = B)
A. Denier B. Twisting
C. Tex D. Pulling
130) ___________ is known as artificial silk. (Answer = A)
A. Rayon B. Acrylic
C. Acetate D. Nylon
131) FTC stands for ________. (Answer = A)
A. Federal Trade commission B. Federal Textile Commission
C. Fata Textile Commission D. Federal Textile Council
132) When we combined different fibers in to yarn is___________ . (Answer = B)
A. Staple B. Blend
C. Cabled D. Decorative
133) The colour of cellulose xanthate in rayon production is. (Answer = C)
A. Blue B. Yellow
C. Orange D. White
134) The construction of knitted fabrics is evaluated by the number of ….. (Answer = C)
A. Holes B. Stitches
C. Loops D. Rings
135) ……………….. fabrics dry very rapidly. (Answer = B)
A. Cotton B. Nylon
C. Wool D. Jute
136) ………….. resistance means dimensional stability in fabric: (Answer = D)
A. Water B. Heat
C. Color D. Shrinkage
137) Jersy fabrics have a tendency to ……….. at the edges: (Answer = A)
A. Curl B. Finish
C. Ravel D. Fix
138) Polyester is normally a ………… fiber: (Answer = C)
A. Rough B. Dull
C. Bright D. Staple
139) Chemical compounds of nylon are classified as …… (Answer = B)
A. Polyvinyl B. Polyamide
C. Estron D. Rubber
140) In weaving, inserting filling yarns through the shed is……… (Answer = B)
A. Shedding B. Picking
C. Battening D. Spinning
141) Number of threads per square inch is………………….in fabric: (Answer = A)
A. Thread count B. Yarn Count
C. Selvage D. Filament
142) ………………… is staple fiber in nature: (Answer = A)
A. Wool B. Silk
C. Rayon D. Orlon
143) Flax is a __________ fiber. (Answer = A)
A. Cellulosic B. Proteinic
C. Synthetic D. Man Made
144) _________is more than just clothing. (Answer = A)
A. Illustrations B. Finishes
C. Fashion D. Sketches
145) _________ was the first designer to have his label sewn into the garments. (Answer = D)
A. Charles Dickens B. Charles James
C. Frederick Jameson Worth D. Charles Frederick Worth
146) ________ is the process of transforming a design in to its constituent flat pattern pieces and then
drafting the out. (Answer = A)
A
A. Pattern making B. Draping
C. Blocks D. Cloth
147) Sisal is a ___________ fiber. (Answer = B)
A. Man made B. Natural
C. Synthetic D. Plastic
148) ________ is the thicker fabric ribbing in the weave. (Answer = A)
A. Taffeta B. Tulle
C. Laces D. Muslin
149) Which of the following is a principle of applying color to yarns? (Answer = B)
A. Digital imaging B. Immersion
C. Bleaching D. None of these
150) China was first producing country of _________ fiber. (Answer = B)
A. Cotton B. Silk
C. Jute D. Flax
151) Which of the following would NOT assist in controlling potential environmental damage caused by the textile industry? (Answer = C)
A. Pollution control B. Government legislation
C. Globalization D. Recycling
152) __________ is technique to create raised design on fabric surface. (Answer = D)
A. Glazing B. Weighting
C. Calendaring D. Embossing
153) Treatment that prevent fabric from clinging. (Answer = C)
A. Water proof finish B. Antibacterial finish
C. Antistatic finish D. Moth proof finish
154) Genesis of textiles means ___________. (Answer = C)
A. Present B. Development
C. History D. Grade
155) APTMA stands for___________. (Answer = A)
A. All Pakistan Textile Mills Association B. All Punjab Textile Manufacturing Association
C. All Power Textile Manufacturing Association D. None of these
156) Bleaching is a __________ treatment. (Answer = A)
A. Whitening B. Mercerizing
C. Cleaning D. None of these
157) Removal of free fiber ends from fabric surface by burning method is __________ . (Answer = C)
A. Cleaning B. Finishing
C. Singeing D. Shearing
158) Red color means the sign of ___________. (Answer = B)
A. Earth B. Danger
C. Rhythm D. All of these
159) _________ are made from chemicals or petroleum and work well in either hard or soft water. (Answer = B)
A. Soaps B. Detergents
C. Bleach D. Starch
160) Other name for screen printing is ___________. (Answer = D)
A. Digital printing B. Transfer printing
C. Synthetic printing D. Silk screen printing
161) C.O.D. stands for _________ . (Answer = B)
A. Care of delivery B. Cash on delivery
C. Care of design D. Collection of delivery
162) Knittiing produce __________ materials. (Answer = A)
A. Stretchable B. Stiff
C. Durable D. None of these
163) Basically hue is the name of ___________. (Answer = D)
A. Pigment B. Dye
C. Paint D. Color
164) __________ is the oldest type of printing. (Answer = B)
A. Screen printing B. Block printing
C. Transfer printing D. Digital printing
165) The yarn count system is used for __________ yarns. (Answer = C)
A. Complex B. Filament
C. Spun D. None of these
166) In dress designing _____ lines are dramatic and more trendy nature. (Answer = C)
A. Vertical B. Horizontal
C. Diagonal D. Curved
167) The extra amount of garment looseness is called (Answer = B)
A. Measurement B. Wearing ease
C. Proportion D. Dis-proportion
168) Self edge of woven fabric is___________. (Answer = A)
A. Selvage B. Bias
C. Dyeing D. Printing
169) There are __________ types of Knitting. (Answer = C)
A. 1 B. 3
C. 2 D. 4
170) Slack yarn is due to ___________ in weaving. (Answer = B)
A. slub yarn B. Insufficient tension
C. Defective yarn D. None of these
171) Ends and picks are known as _________ and __________ respectively. (Answer = A)
A. Warp and filling B. Filling and warp
C. None of these D. Both of these
172) Part of the garment that turns back below the collar is called __________. (Answer = C)
A. Yoke B. Hem
C. Lepel D. Trim
173) __________ technique is used to prevent the edge from fraying. (Answer = B)
A. Seam allowance B. seam Finish
C. Seam D. none of these
174) When the design elements work well together __________ is achieved. (Answer = D)
A. Rhythm B. Balance
C. Proportion D. Harmony
175) Lightness or darkness of color is called ___________. (Answer = B)
A. Shade B. Value
C. Tint D. None of these
176) The outline or silhouette of an object is called __________. (Answer = A)
A. Shape B. Space
C. Proportion D. Rhythm
177) The pleasing arrangement of all parts of garment is called ___________. (Answer = B)
A. Balance B. Harmony
C. Proportion D. Rhythm
178) In knitting warp knits are made with __________ Yarns. (Answer = D)
A. One B. Four
C. Three D. Several
179) Regenerated fibers are widely used in___________. (Answer = B)
A. Clothing B. Industries
C. Carpets D. Nets
180) The decorative art of tying knots is called ——————. (Answer = A)
A. Macrame ́ B. Crocheting
C. Braiding D. Embroidery
181) When two or more yarns are twisted together they are designated as ————- yarns. (Answer = C)
A. Doubled B. Novelty
C. Ply D. Cabled
182) Fashion also affects noneconomic matters as __________. (Answer = D)
A. Money B. Economy
C. Expenses D. Social customs
183) Important trimmings used to decorate garment are__________. (Answer = D)
A. Flayers B. Nets
C. Knits D. Laces
184) —————– is used in mercerization. (Answer = A)
A. Sodium hydrooxide B. Schreinerizing
C. Glactose D. None of these
185) The strength, abrasion resistance and stability of polyester make it very suitable for_________. (Answer = B)
A. Ropes B. Sewing thread
C. Pampers D. Industries
186) Batik is a technique of __________. (Answer = B)
A. Dye resist dyeing B. Wax resist dyeing
C. Tie and dye D. Block resist dyeing
187) Spinnerete orfices are coated with specific__________. (Answer = C)
A. Solution B. Tank
C. Alloy D. Net
188) Fabric is treated with heat and pressure to add luster. (Answer = A)
A. Lustering B. Felting
C. Beetling D. Glazing
189) The ability of fiber to stretch and return to shape is……(Answer = A)
A. Elasticity B. Crimp
C. Stretch D. Pliability
190) Disposable masks are made by __________. (Answer = A)
A. Polypropylene B. Paper
C. Jute D. None of these
191) In fabrics charge develop from friction by wearing and general use is _________. (Answer = A)
A. Static charge B. Friction
C. Slipping D. None of these
192) How many operations are fundamental in any type of weaving? (Answer = B)
A. 03 B. 04
C. 05 D. 06
193) The right-hand twist is called. (Answer = C)
A. Twist B. S twist
C. Z twist D. None of these
194) A sketch can be turned into a __________. (Answer = B)
A. Design B. Garment
C. Picture D. Fabric
195) The length of measuring tape is __________. (Answer = C)
A. 50 inches B. 62 inches
C. 60 inches D. 59 inches
196) A garment is a ___________ product. (Answer = B)
A. Two dimensional B. Three dimensional
C. Four dimensional D. Six dimensional
197) Garment cutting and manufacturing is based on…… (Answer = A)
A. Measurements B. Fit
C. Style D. Fullness
198) __________ are added for movement to make the garment comfortable to wear. (Answer = B)
B A. Seam allowance B. Ease allowance
C. Hem allowance D. Fasteners
199) Rayon is made of …….. (Answer = A)
A. Cellulose B. Oxygen
C. Flax D. Coal
200) The only natural fiber that may be a filament……. (Answer = B)
A. Polyester B. Silk
C. Cotton D. Linen
201) Clothing labels are
C A. Identify fabric contents B. Required by law
C. Both D. None of these
202) Fabric surface can be raised by ___________ finish. (Answer = A)
A. Napping B. Bleaching
C. Wetting D. Stretching
203) Stain must be removed as early as it is ___________. (Answer = B)
B A. Fixed B. Fresh
C. Dry D. Darker
204) Which type of selvage is made of heavier yarns or ply yarns to provide greater strength to fabric: (Answer = B)
A. Plain B. Tape
C. Split D. Fused
205) The process of making yarn from fiber is called. (Answer = A)
A. Bobbin B. Handloom
C. Moth D. Needle
220) Silk, the natural form of fiber is obtained from…..(Answer = B)
A. Sheep B. Cocoon
C. Jute plant D. Cotton balls
221) Which type of weave is suitable for printing purpose? (Answer = A)
A. Plain B. Basket
C. Satin D. Twill
222) Which of the following statements is not true about wool- A natural form of fiber? (Answer =B)
A. Wool fiber is obtained from sheep B. Wool fiber is obtained from moth
C. Wool fiber is obtained from llama D. Wool fiber is obtained from alpaca
223) The size relationship of each of the internal spaces within a garment to one another and to the total look is ___________ . (Answer = D)
A. Rhythm B. Shape
C. Harmony D. Proportion
224) The property of a fabric which determines its feels, looks and moves when it is worn is_________ . (Answer = A)
A. Texture B. Shape
C. Weave D. Crimp
225) Fabric as it comes from the loom before it is finished is called___________ . (Answer = C)
A. Mercerized B. Bleached
C. Grey goods D. Textured
226) All the decisions that go into the selling of a product called. (Answer = A)
A. Market Research B. Marketing
C. Merchandizing D. Planning
227) Which finish is used to increase the absorption of nylon fabrics? (Answer = C)
A. Embossing B. Mercerization
C. Nylonizing D. Molding
228) High denier count give__________ to the fabrics. (Answer = A)
A. Strength B. Elasticity
C. Crimp D. Shine
229) The property of fiber bending without breaking is __________. (Answer = C)
A. Spinning quality B. Tenacity
C. Flexibility D. Breaking strength
230) Non-woven fabric is made by ______________ process. (Answer = D)
A. Yarn B. Fiber
C. Cloth D. Felting
231) Count Hilaire de Chardonnet was known as the father of ____________. (Answer = A)
A. Rayon B. Acetate
C. Nylon D. Polyester
232) The fabric of compact construction has a ____________Thread count: (Answer = C)
A. Low B. Medium
C. High D. Equal
233) Possible deficiencies in clothing itself may include (Answer = D)
A Stains B. Smell
C Holes D. All of these
234) Highly labor intensive for apparel is its ___________ . (Answer = A)
A Production B. Wearing
C Discarding D. Consumption
235) The quickest and easiest way to make a garment is___________ . (Answer = A)
A. Draping B. Weaving
C. Knitting D. None of these
236) The process that uses special liquids containing solvents to clean fabrics. (Answer = B)
A Solvent B. Dry cleaning
C Laundering D. Agitation
237) When fabric permanently joined to other fabric on material means__________. (Answer = B)
A. Blended B. Bonded
C. Woven D. Wales
238) Through increasing rates of recycling, we decrease the levels of ___________. (Answer = B)
A. Air B. Waste
C. Material D. Business
239) Benefits of Recycling has not only for business but also for___________. (Answer = C)
A. Institute B. Home
C. Environment D. Saving
240) The fibers with polyamide groups are called ___________ . (Answer = A)
A. Nylon B. Polyester
C. Rayon D. Spandex
241) Nylon is one of the lightest fiber with good ___________ . (Answer = B)
A. Abrasion B. Strength
C. Weight D. Apsorption
242) A cellulosic fiber usually made from wood pulp __________ . (Answer = C)
A. Nylon B. Cotton
C. Rayon D. Orlon
243) Final stage in spinning is ____________. (Answer = B)
A. Carding B. Cone winding
C. Mixing D. Opening
244) Fancy and decorative yarns used in textiles are ___________. (Answer = B)
A. Cabled B. Novelty
C. Spun D. Staple
245) Along each edge of woven fabric, there is a___________. (Answer = B)
A. Stripe B. Selvage
C. Color D. Yarn
246) The variation of plain weave is____________. (Answer = D)
A. Twill B. Sateen
C. Satin D. Basket
247) Rayon fiber manufactured through___________ spinning process. (Answer = A)
A. Wet B. Dry
C. Melt D. Ring
248) Now a days people prefer the way of shopping . (Answer = C)
A. Land B. Shipping
C. Online D. None of these
249) The economics of clothing involve production, distribution and___________ . (Answer = A).
A. Consumption B. Radiation
C. Management D. Fashion
250) Linen fiber first grew by the __________civilization. (Answer = B)
A. Chinese B. Egyptian
C. Victorian D. Indians
251) All bleaching processes—————–the strength of fiber: (Answer = B)
A. Increase B. Decrease
C. No Change D. None of these
252) The textile sector contributing—————–to the country’s exports: (Answer = B)
A. 47% B. 67%
C. 87% D. 40%
253) Fibers less than 1 denier per filament in length are called —————— fibers. (Answer = D)
A. Macrofibres B. Long length fibers
C. Filament Fibers D. Microfibers
254) While wet, wool may lose as much as —————- percent of its strength. (Answer = B)
A. 50% B. 25%
C. 40% D. 70%
255) ———————- is a Portion of garment that spreads out or widens. (Answer = A)
A. Flare B. Bodice
C. Flap D. None
256) —————-is the transfer of construction symbols from paper pattern to fabric. (Answer = D)
A. Matching B. Joining
C. Lining D. Marking
257) The ability of a fabric to hang and fall into graceful shape and folds is called ——————. (Answer = C)
A. Strength B. Flexibility
C. Drape D. None
258) The desirable folds in the fabric are called———————-. (Answer = A)
A. Creases B. Wrinkles
C. Both a & b D. None
259) Cutting chart on instruction guide sheet showing the placement of pattern pieces is called———. (Answer = C)
A. Marking B. Motif
C. Layout D. None
260) ——————– means the fray in the cutting edges of the fabric. (Answer = A)
A. Ravel B. Bias
C. Notch D. Placket
261) The extra amount of garment looseness is called———————. (Answer = B)
A. Measurement B. Wearing Ease
C. Proportion D. Dis-proportion
262) ——————–means the width of fabric beyond the seam line, not including the garment area. (Answer = B)
A. Garment Allowance B. Seam Allowance
C. Fabric Allowance D. None
263) The loss of color, when dyed fabric is immersed in water is called ——————–. (Answer = B)
A. Crocking B. Bleeding
C. Shading D. Barre
264) —————— is the weakest of natural fibers. (Answer = C)
A. Cotton B. Linen
C. Wool D. Silk
265) The ability of a fibre to hang easily and fall into graceful shapes indicates its ———–. (Answer = C)
A. Resilience B. Elasticity
C. Drapability D. Both B & C
266) Indigo was the first synthetic ———— dye. (Answer = A)
A. Vat B. Azoic
C. Disperse D. Reactive
267) The process of dyeing at ————- stage is called Stock dyeing. (Answer = A)
A. Fiber B. Fabric
C. Yarn D. Filament
268) The ability of a color to remain unchanged is called ——————.(Answer = A)
A. Color Flare B. After Chroming
C. Colorfastness D. Color bleeding
269) In any type of weaving there are ———— fundamental operations. (Answer = D)
A. 3 B. 2
C. 5 D. 4
270) —————– weave is the most durable and strong weave. (Answer = C)
A. Basket B. Satin
C. Twill D. Plain
271) Interlacing of two sets of yarns is called——————-. (Answer = B)
A. Knitting B. Weaving
C. Crocheting D. None of these
272) —————– is a vegetable fibre. (Answer = D)
A. Silk B. Wool
C. Polyester D. Cotton
273) – Charles Worth was the first ———–, who designed dresses for French royal family. (Answer = A)
A. Fashion designer B. Textile designer
C. Entrepreneurer D. None
274) ————— is an inexpensive method for imparting luster to low-priced cottons. (Answer = B)
A. Calendaring B. Schreinerizing
C. Glazing D. None of these
275) a Sewing one or more pieces of fabric to the top of a large piece of fabric is called—————. (Answer = A)
A. Applique B. Patchwork
C. Felting D. Quilting
276) All the decisions that go into the selling of a product called——————. (Answer = C)
A. Market Research B. Marketing
C. Merchandising D. All of these
277) The raised surface on a fabric is called—————-.(Answer = A)
A. Pile B. Texture
C. Pill D. None of these
278) The outline or silhouette of an object is called—————-. (Answer = A)
A. Shape B. Space
C. Proportion D. Rhythm
279) In the weaving operations, inserting filling yarns through the shed is called—————. (Answer = B)
A. Shedding B. Picking
C. Beating up D. Taking up
280) The decorative art of tying knots is called —————-. (Answer = A)
A. Macrame ́ B. Crocheting
C. Braiding D. Embroidery
281) Mercerizing process increases the strength of cotton as much as ————- . (Answer = B)
A. 40% B. 20%
C. 10% D. 50%
282) A garment labeled as “—————” will provide protection from moderate rain for many hours. (Answer = A)
A. Rain resistant B. Water repellent
C. Water resistant D. None
283) A garment labeled as “Rain resistant” will provide protection from moderate rain for ———- . (Answer = B)
A. Many hours B. Few hours
C. fifteen minutes D. one day
284) —————- is an ironing process that adds sheen to the fabric. (Answer = C)
A. Glazing B. Weighting
C. Calendaring D. Embossing
285) A public promotion of some product or service is called ——————. (Answer = C)
A. Marketing B. Merchandising
C. Advertisement D. All of above
286) The approach a company uses to identify its customer’s needs and the company’s ability to satisfy those needs is called——————. (Answer = C)
A. Marketing Mix B. Marketing Concept
C. Marketing Strategy D. Marketing Environment
287) Which of the following is a social value? (Answer = B)
A. Power B. Love
C. Unity D. Truth
288) The companies that provide raw materials for Fashion Pipeline are called —————. (Answer = B)
A. Finish Product Supplier B. Component Supplier
C. Retail Distributor D. None of These
289) Any style that we have grown tired of looking at is called ——————. (Answer = D)
A. Tradition B. Classic
C. Fad D. Old-fashioned
290) The less expensive copies of designer’s garments are called————-. (Answer = A)
A. Knock-off B. Seconds
C. B-Grade D. None of these
291) Darkness of a color is known as ..….(Answer = A)
A. Shade B. Tint
C. Intensity D. Brightness
292) A substance used to dissolve another substance is called —————. (Answer = C)
A. Solution B. Solute
C. Solute D. Solvent
293) Loose fabric is also known as —————. (Answer = A)
A. Cloth B. Yarn
C. Fibre D. String
294) Dye is added to the chemical solution before it is forced into manufactured fibres, called ———. (Answer = A)
A. Solution Dyeing B. Top dyeing
C. Yarn dyeing D. Stock Dyeing
295) The term used for items worn on the body is called—————. (Answer = A)
A. Clothes B. Wearing
C. Garments D. Dresses
296) When two or more yarns are twisted together they are designated as ————– yarn. (Answer = C)
A. Doubled B. Novelty
C. Ply D. Cabled
297) —————— means that the store owner will put the items on sale in the store. (Answer = A)
A. Consignment B. Shipment
C. Promotion D. Marketing
298) The fabric come out from the loom is known as….(Answer = C)
A. White goods B. Black goods
C. Grey goods D. None
299) Fabric as it comes from the loom before it is finished is called ————–. (Answer = B)
A. Bleached B. Grey goods
C. Mercerised D. None
300) Fashion industry has always been very_________ because of large companies competing. (Answer = C)
A. Decline B. Powerful
C. Competitive D. Strong
301) How a fabric handles and feels————-. (Answer = B)
A. Elasticity B. Texture
C. Crimp D. Stretch
302) Dyes are the compounds that ————– textile. (Answer = C)
A. Bleach B. shrink
C. Color D. None
303) Jute is a —————- fibre. (Answer = A)
A. Plant B. Animal
C. Synthetic D. Man made
304) Crafts that are created by using your hands are called————–. (Answer = A)
A. Handicrafts B. Design
C. Hand works D. Drawings
305) The ability of a fibre to stretch and return to shape is called——————-.(Answer = C)
A. Resiliency B. Shrinkage
C. Elasticity D. None
306) Calendaring is an ironing process that adds————– to the fabric. (Answer = C)
A. Texture B. Weight
C. Sheen D. None
307) Component suppliers provide —————- materials for Fashion Pipeline. (Answer = B)
A. Finished Material B. Raw Material
C. All Material D. None
308) Different fibers combined in to one yarns ——————–. (Answer = C)
A. Bonded B. Filling
C. Blends D. Weaving
309) The ability of a fabric to withstand tension or pulling is called. (Answer = D)
A. Shape Retention B. Abrasion
C. Resiliency D. Tensile Strength
310) When heat and moisture are applied to wool, the scales spread and soften slightly. (Answer = B)
A. Compression B. Felting
C. Calendaring D. None
311) Triangular-shaped folds of fabric stitched to control fullness are called —————. (Answer = C)
A. Gathers B. Pleats
C. Darts D. Hems
312) In a knit, the widthwise rows of stitches are called——– . (Answer = A)
A. Courses B. Wales
C. Warps D. None
313) —————– is a whitening treatment. (Answer = B)
A. Mercerising B. Bleaching
C. Calendaring D. None
314) —————- is a finishing treatment. (Answer = D)
A. Dyeing B. Printing
C. Cleaning D. Sizing
315) .The designer of ——————-show a new collection twice a year. (Answer = B)
A. Pret A porter B. Haute Couture
C. Both a & b D. None
316) The combination of a primary color with a secondary color is called—————– color. (Answer = D)
A. Complementary B. Neutral
C. Triad D. Intermediate
317) Anything that wear, cover and adorns the body is called …..(Answer = C)
A. Textile B. Designing
C. Clothing D. Dressing
318) A fashion that is very popular for a short time is called ————–. (Answer = C)
A. Classic B. Style
C. Fad D. Tradition
319) The direction of threads in a —————– fabric is known as Grain. (Answer = D)
A. Printed B. Dyed
C. Crocheted D. Woven
320) ——————-of yarn means twisting. (Answer = C)
A. Weaving B. Glazing
C. Spinning D. Printing
321) Artificial silk is————–. (Answer = A)
A. Rayon B. Acetate
C. Cotton D. Wool
322) The first fashion designer was——– (Answer = C)
A. Robertson B. Shakespeare
C. Charles Frederick Worth D. Ellie Saab
323) Linen is obtained from (Answer = A)
A. Flax B. Cotton
C. Jute D. None
324) The process used to increase the luster of cotton is called —————-. (Answer = B)
A. Bleaching B. Mercerization
C. Nylonizing D. Napping
325) Surface ornamentation of fabric is called (Answer = B)
A. Fashion Designing B. Textile Designing
C. Dyeing D. None
326) A tall slender plant that is used to make linen fabric is called—————–. (Answer = A)
A. Flax B. Cotton
C. Silk D. Wool
327) An instrument used to weave the crosswise threads on a loom is called—————. (Answer = B)
A. Cloth beam B. Shuttle
C. Harness D. Heddles
328) —————-shaped folds of fabric stitched to control fullness are called darts. (Answer = B)
A. Rectangular B. Triangular
C. Square D. Circle
329) The process of converting fibers directly into fabric is (Answer = C)
A. Weaving B. Spinning
C. Felting D. Knitting
330) —————– is the group of individuals who live together in a particular area (Answer = C)
A. Heritage B. Culture
C. Society D. None
331) ——————— is the formation of bunches or balls of tangled fibres on the surface of fabric. (Answer = A)
A. Pilling B. Abrasion
C. Pile D. None
332) Red, yellow and blue are —————— colors (Answer = C)
A. Neutral B. Cool
C. Primary D. Secondary
333) Neutral colors are—————— (Answer = A)
A. Black & White B. Red & Green
C. Yellow & Pink D. None
334) Physical count of merchandise is ——————. (Answer = C)
A. Sheet B. Frame
C. Inventory D. Versatile
335) Thread count of woven fabric is —————– per inch of woven fabric is known as (Answer = A)
A. Threads per square inch B. Fibres per square inch
C. Fabric per square inch D. None
336) The microscopic structure of ____________ fiber looks like a bamboo pole. (Answer = A)
A. Flax B. Cotton
C. Silk D. Wool
337) —————— of woven fabric is called selvage. (Answer = B)
A. Center B. Self edge
C. Right edge D. Left edge
338) Cotton is a ____________fiber. (Answer = A)
A. Artificial B. Plant
C. Animal D. The plumber and the painter work on consecutive days.
339) In —————– warp knits are made with several yarns. (Answer = D)
A. Printing B. Knitting
C. Weaving D. Dyeing
340) Application of heat and ——————— on wool, to soften the scales is called felting. (Answer = C)
A. Pressure B. Temperature
C. Moisture D. None
341) The decorative art of —————— is called macramé. (Answer = A)
A. Tying knots B. weaving
C. Crocheting D. None
342) The process of removing the starch from the fabric is called ——————-.(Answer = C)
A. Bleaching B. Mercerizing
C. Desizing D. none
343) Inner hollow hole of cotton fiber is known as (Answer = C)
A. Serine B. Lint
C. Lumen D. Pectin
344) Metallic fibers are only used for (Answer = A)
A. Strength B. Apparel
C. Decoration D. None of these
345) Exclusive or specialized designed dresses are (Answer = C)
A. Pret a porter B. Bridal couture
C. Haute couture D. None
346) Beetling is a finish applied to linen fabrics, in which fabric is beaten with___________ hammer. (Answer = B)
A. Iron B. wooden
C. Copper D. steel
347) ——————- finish is used to keep the fabric flat and smooth. (Answer = A)
A. Wrinkle resistant B. Shape Retentive
C. Water repellent D. Flame retardent
348) Finishes are classified according to their degree of_____________ . (Answer = C)
A. Temporary B. Semi durable
C. Permanence D. none
349) All cotton fabrics are singed except those that are______________. (Answer = B)
A. Bleached B. Napped
C. Shrinked D. Dyed
350) The success or failure of the fashion industry depends on__________ purchases of its products. (Answer = C)
A. Retailers B. Sellers
C. Consumers D. None
351) The area inside the shape is called ——————–. (Answer = B)
A. Color B. Space
C. Texture D. None of these
352) The ability of fabric to draw moisture away from your body is———————: (Answer = B)
A. Wicking B. Absorbency
C. Resiliency D. none
353) When twist is increased in the spun yarn, its strength————–: (Answer = D)
A. Increases B. Decreases
C. Does not change D. First increases then decreases
354) Filament yarns are——————–: (Answer = B)
A. Short length B. Long length
C. Medium length D. None
355) Sunlight is the principle bleaching aid for fine——————-: (Answer = C)
A. Cotton B. Linen
C. Polyester D. Silk
356) Indigo was the first————- vat dye: (Answer = B)
A. Natural B. Synthetic
C. Both A & B D. None
357) Denier is the term applied to the —————- of yarn. (Answer = C)
A. Resiliency B. Elasticity
C. Strength D. None
358) ———————- processes are undertaken by highly specialized companies called converters. (Answer = C)
A. Dyeing B. Printing
C. Finishing D. None
359) A __________ is a device, sign or name that is used to identify the product. (Answer = A)
A. Brand B. Price
C. Botique D. Color
360) Caustic soda mercerization of cotton is carried out for improvement of (Answer = A)
A. Strength & Luster B. Whiteness
C. Wetting D. Absorption
361) Warp faced satin is____ than the weft faced sateen. (Answer = D)
A. Lustrous B. Rough
C. Weaker D. Stronger
362) Water jet looms are capable of inserting ______________. (Answer = A)
A. 700 picks per minute B. 75 picks per minute
C. 180 picks per minute D. 45 picks per minute
363) Which of the following is the odd one out with regards to enhancing whiteness in textile material? (Answer = D)
A. Bleaching B. Optical Brightener
C. Bluing agent D. Alkali
364) Why azoic dyes are also called ice colours? (Answer = B)
A. As they develop cool colours of blue and green
B. Ice is used to maintain the temperature as low as 0-5 Deg Centigrade
C. They were first discovered by Perkin in the polar regions.
D. The dye particles resemble ice crystals
365) ______________is a style that is popular in the present or a set of trends that has been accepted by a wide audience. (Answer = C)
A. Style B. Fad
C. Fashion D. Classic
366) In which stage of the fashion cycle do consumers reject a style and start looking out for something
new (Answer = D)
A. Decline B. Introduction
C. Peak D. Rejection
367) The traditional process of fashion adoption is also called as (Answer = A)
A. Trickle Down B. Trickle Up
C. Trickle Across D. Mass Dissemination
368) ______________ create fashion. (Answer = D)
A. Fashion role models B. Fashion followers
C. Fashion Victims D. Fashion Innovators
369) Hoodies come under which wear (Answer = B)
A. Party wear B. Casual wear
C. Swim wear D. Formal wear
370) Which is not a type of marketing concept? (Answer = D)
A. The production concept B. The selling concept
C. The social marketing concept D. The supplier concept
371) This tool is used to temporarily hold two or more pieces of fabric together. (Answer = B)
A. Chalk B. Pins
C. Bobbins D. Needles
372) This is a guide containing steps to make a garment. (Answer = D)
A. Thimble B. Needle threader
C. Sewing gauge D. Pattern
373) This tool protects your fingers when you sew by hand. (Answer = A)
A. Thimble B. Sewing gauge
C. Thread D. Rotary cutter
374) Strength of the cotton increases with (Answer = B)
A. Decrease in moisture content B. Decrease in moisture content
C. Increase in temperature D. Decrease in relative humidity
375) A ——————– is the secondary property of textile fibers. (Answer = B)
A. Strength B. Fineness
C. Weight D. Length
376) The process of supplying necessary moisture to textile is (Answer = C)
A. Weighting B. Scouring
C. Conditioning D. Tinting
377) The ratio of actual vapor pressure to the maximum vapor pressure, expressed as a percentage is
called- (Answer = C)
A. Absolute humidity B. Moisture Regain
C. Relative Humidity D. Moisture Content
378) ———— is the natural mineral fiber. (Answer = A)
A. Asbestos B. Glass
C. Nylon 6 D. Aramid
379) Singeing removes —————– fibers (Answer = C)
A. Protein B. Vegetable
C. Protruding D. Entangled yarns
380) ————- has excellent elastic recovery. (Answer = C)
A. Cotton B. Polyester
C. Nylon D. Viscose
381) ————– has excellent crease resistance. (Answer = B)
A. Cotton B. Polyester
C. Nylon D. Viscose
382) The hollow space in cotton is known as ——————. (Answer = A)
A. Lumen B. Medulla
C. Pores D. Stomas
383) The protein present in wool is —————. (Answer = B)
A. Elastin B. Keratin
C. Fibronectin D. Kevlar
384) The species that yield mulberry silk is ——–. (Answer = B)
A. Philosamia ricinis B. Bombyx mori
C. Antheraea paphis D. Anthraea assamia
385) The substance removed during degumming is ——————-. (Answer = A)
A. Sericin B. Fibroin
C. Natural coloring matters D. Wool wax
386) —————– dyes are readily soluble in water. (Answer = B)
A. Naphthol B. Reactive
C. Disperse D. Sulphur
387) Mercerization of cotton is carried out for————— (Answer = A)
A. Strength & Luster B. Whiteness
C. Wetting D. None
388) The only natural fiber that may be a filament is ———– (Answer = B)
A. Cotton B. Silk
C. Polyester D. Linen
389) Rayon is made of —————— (Answer = D)
A. Coal B. Oxygen
C. Flax D. Cellulose
390) Scouring of cotton is carried out under (Answer = A)
A. Alkaline conditions B. Acidic conditions
C. Neutral conditions D. None
391) When twist is increased in a spun yarn, its strength (Answer = D)
A. increases B. Decreases
C. Does not change D. First increases then decreases
392) The most important ingredient of a scouring composition is (Answer = B)
A. Wetting agent B. Alkali
C. Emulsifying agent D. Sodium silicate
393) Mercerization is carried out with NaOH of (Answer = B)
A. 10 –15% Conc. B. 18 –25% Conc.
C. 5 –10% Conc. D. 25-35% Conc.
394) An optical brightener is (Answer = B)
A. A synthetic bluing agent B. A colorless dye
C. A fluorescent compound D. An optical whitener
395) The most productive method for textile printing is (Answer = A)
A. Rotary screen printing B. Automatic Flat-bed screen printing
C. G Block printing D. None
396) Spun yarns are——- (Answer = C)
A. Smooth B. Lustrous
C. Dull D. Cool
397) Filament yarns are————– (Answer = A)
A. Smooth B. Dull
C. Soft D. Short
398) Novelty yarns are usually—————— (Answer = C)
A. Boucle Yarns B. Textured Yarns
C. Ply yarns D. Card yarns
399) Spinning of yarn means——— (Answer = B)
A. Denier B. Twisting
C. Tex D. Pulling
400) —————– weave produces lustrous surface. (Answer = B)
A. Twill B. Satin
C. Jacquard D. Pile
401) —————- fiber is used to create linen. (Answer = B)
A. Cotton B. Flax
C. Wool D. Silk
402) —————- refers to the amount of roominess in a garment. (Answer = C)
A. Grain line B. Dart
C. Ease D. Tuck
403) ——————– is the process of transforming designs to its constituent flat pattern pieces and then
drafting them out. (Answer = A)
A. Pattern making B. Draping
C. Template D. Blocks
404) What should be minimum length of fibers for making of yarn from fiber? (Answer = B)
A. One inch B. Half inch
C. One centimeter D. Half centimeter
405) How many types the fibers have been classified based on the length of the fiber staples? (Answer = B)
A. Two Types B. Three Type
C. Four Types D. Five Types
406) Which one is the most important quality of textile fiber? (Answer = A)
A. Fineness B. Moisture Content Value
C. Length D. Cohesiveness power
407) Which one is the protein fiber? (Answer = D)
A. Cotton B. Jute
C. Rayon D. Silk
408) What is the Moisture regain value of cotton fiber? (Answer = C)
A. 7% B. 8%
C. 8.5% D. 9%
409) As the length of —————- fiber increases, its fineness also increases. (Answer = D)
A. Silk B. Jute
C. Wool D. Cotton
410) The cross sectional shape of —————– fiber looks triangular? (Answer = B)
A. Jute B. Silk
C. Wool D. Nylon
411) —————fiber melts in excessive heat. (Answer = B)
A. Silk B. Polyester
C. Jute D. Cotton
412) Which is the best cotton fiber? (Answer = B)
A. Egyptian B. Seguisland
C. Indian D. American
413) What type of smell is felt during burning of cotton fiber? (Answer = A)
A. Paper burning
B. Feather burning
C. Hair burning
D. No Smell
414) ————— fiber is damaged by acid. (Answer = D)
A. Polyester B. Acrylic
C. Wool D. Cotton
415) Which fiber is the alternative to wool? (Answer = D)
A. Cotton B. Polyester
C. Nylon D. Acrylic
416) Which elements are used in making viscose rayon fiber? (Answer = D)
A. Oil and water B. Coal and air
C. Oil and coal D. Wood and bamboo
417) What is meant by yarn count? (Answer = D)
A. Counting of yarn B. Strength of yarn
C. Density of yarn D. Thickness of yarn
418) The steaming of cotton yarn is done for————— (Answer = C)
A. increasing the strength of yarn B. increasing the weight of yarn
C. setting of twist of yarns D. increasing the glaze of the yarn
419) Combed yarns are better than carded yarns because———– (Answer = B)
A. All say it is good B. Quality
C. Price is higher D. Price is lower
420) Why are the ends/inch kept greater than the picks/inch in fabrics? (Answer = A)
A. The cost is lower B. The fabrics look good
C. As it is mandatory D. Fabrics become more stronger
421) Minimum how many frames are required for producing plain fabrics? (Answer = A)
A. 2 B. 3
C. 4 D. 5
422) Primary motion of a weaving machine is ——————— (Answer = A)
A. Shedding, picking and beat-up B. Shedding and picking
C. Picking and beat-up D. Let-off and take-up
423) Why is starch used in warp yarn? (Answer = B)
A. To increase the luster of the yarn B. To increase the strength of yarn
C. For smoothing the yarn D. For increasing the weight of the warp yarn
424) Why are the picks/inch kept smaller than the ends/inch in fabrics? (Answer = A)
A. Cost comes lower B. Cost comes higher
C. Fabrics look good D. The quality of fabric increases
425) ——————– is the secondary motion of a weaving machine. (Answer = D)
A. Shedding B. Picking
C. Warp protector mechanism D. Let-off motion
426) —————— is not a weaving fault. (Answer = D)
A. Shuttle mark B. Reed mark
C. Running stripe D. Oil spot
427) —————— type of fabric is produced by jacquard weaving machine. (Answer = D)
A. Plain B. Twill
C. Zig zag D. Fabric with big designs.
428) GSM of a fabric means —————- (Answer = C)
A. The construction of fabric B. The strength of fabric
C. The weight of fabric D. Thickness of fabric
429) ————————-dye is used for dyeing of polyester fabrics. (Answer = D)
A. Direct dye B. Vat dye
C. Reactive dye D. Disperse dye
430) ————————-dye is not used for dyeing of Cotton fabrics. (Answer = D)
A. Reactive B. Sulfur
C. Vat D. Disperse
431) ——————–dye allows better colorfastness to cotton fabrics. (Answer = C)
A. Direct B. Reactive
C. Vat D. Sulfur
432) Why is scouring done for cotton fabrics? (Answer = D)
A. For removing starch B. For setting dimension
C. For increasing strengths D. For removing garbage from cotton fibers
433) Generally, which type of printing is not used in fabric printing? (Answer = D)
A. Block print B. Batik print
C. Roller print D. Transfer print
434) ————- dye gives the lowest cost for dyeing. (Answer = A)
A. Direct Dye B. Reactive Dye
C. Vat Dye D. Acid Dye
435) Stentering machine is used to ————- (Answer = A)
A. Drying of fabric and setting of dimension B. To print fabric
C. To clean fabric D. To control fabric shrinkage
436) ——————- agent is used for bleaching of fabrics. (Answer = C)
A. De-singeing material B. Acid
C. Hydrogen peroxide D. Potassium permanganate
437) Pilling occur in fabric————– (Answer = C)
A. If fabric is dirty B. If fabric is much used
C. Much hairy fiber in fabric D. If fabric is less used
438) Singeing done in fabrics for ————— (Answer = C)
A. Cleaning of fabrics B. Thinning of fabrics
C. Removing hairy fibers from fabrics D. Setting of dimension in fabrics
439) ————-test is not required for testing of the fiber. (Answer = C)
A. Strength test B. Length test
C. Crease Recovery test D. Humidity Test
440) Staple length of fibers means ————– (Answer = D)
A. Average length B. Maximum length
C. Minimum length D. Modal length
441) What happens in pre-treatment? (Answer = B)
A. Fabric weight increases B. Fabric weight decreases
C. Fabric weight remains unchanged D. Fabric length increases
442) Drape test of fabric is done for————– (Answer = C)
A. For examining weight of fabrics B. For examining thickness of fabrics
C. For examining hanging behavior of fabrics D. For examining strength of fabrics
443) Which one of the below tests is not done for testing of yarn? (Answer = B)
A. Strength B. Pilling
C. Count D. Hairiness
444) Micronaire means——————- (Answer = C)
A. Fineness of yarn B. Fineness of fabric
C. Fineness of fiber D. Construction of fabric
445) Cross-sectional shape of Viscose Rayon is ————— (Answer = C)
A. Round B. Rectangular
C. Star shape D. Ribbon shape
446) The length of a silk fiber is ————– (Answer = A)
A. 400 to 700 meter B. 400 to 500 meter
C. 500 to 600 meter D. 500 to 700 meter
447) Why is Doubling done in yarn manufacturing? (Answer = B)
A. For elongating the material B. For decreasing the irregularities of material
C. For decreasing the slub problem D. For controlling the hairiness of yarn
448) What has been meant by Marker in garments industry? (Answer = C)
A. One kind of pen B. One kind of label
C. The paper for drawing the pictures of patterns D. Colored sticker for marking garments
449) What has been meant by Seam Pucker? (Answer = B)
A. The holes in seams B. Creasing of fabrics along the seams
C. Types of seam D. Length of seam
450) What is meant by Grading in garments industry? (Answer = C)
A. To classify the garments based on quality B. To classify the garments based on sizes
C. To make patterns of various sizes D. To make patterns of various designs
451) What is meant by Fusing in garments industry? (Answer = C)
A. Paper interlining B. Sewn interlining
C. Joining of interlining through heat and pressure D. None
452) Crease Mark happen in fabric during (Answer = C)
A. Using of garments B. Ironing
C. Dyeing D. Cleaning of garment
453) With an increase of moisture content, the strength of a Nylon filament —————- (Answer = B)
A. Increases B. Decreases
C. First increases then decreases D. First decreases then increases
454) Modifications in clothing reflect (Answer = D)
A. grace and beauty B. ideas of modesty
C. ideas of shame D. change in societies
455) Colour of the cap of Liberty worn by French revolutionaries was (Answer = A)
A. Red B. Green
C. White D. Yellow
456) During medieval times Bloomers were————— (Answer = B)
A. Knickers B. Trousers
C. Short skirts D. Tunics
457) Which among the following Indian population were the first to adopt western styles? (Answer = A)
A. Men B. Women
C. Children D. Bengalis
458) A primary property of a textile fiber which refers to adequate strength is ————— (Answer = D)
A. cohesiveness B. Flexibility
C. Density D. Tenacity
459) Find the odd one out? (Answer = D)
A. Cotton B. Jute
C. Linen D. Silk
460) Fibers that are measured in centimeters or inch are? (Answer = A)
A. Staple fibers B. Filament fibers
C. Short fibres D. Long fibres
461) Tenacity is the term usually applied to the strength of? (Answer = A)
A. Fiber B. Yarn
C. Fabric D. Cotton
462) Denier is the term applied to the strength of? (Answer = B)
A. Fiber B. Yarn
C. Fabric D. Cotton
463) ——————— is the property of bending without breaking. (Answer = B)
A. Bending strength B. Flexibility
C. Spinning quality D. Tenacity
464) Cohesiveness is also termed as——————— (Answer = A)
A. Spinning quality B. Uniformity
C. Flexibility D. Tenacity
465) Density is expressed as ——————– (Answer = B)
A. mass per unit volume B. relative mass per unit volume
C. none of the above D. Both a and b
466) The primary property essential for a fiber is——————— (Answer = C)
A. Luster B. density
C. length to width ratio D. resiliency
467) The ability of a fiber to return to shape is —————– (Answer = C)
A. Elastic recovery B. Elongation
C. Resiliency D. Spinning quality
468) When the fibre molecules are arranged in random then it is ——————- (Answer = D)
A. high orientation B. Low orientation
C. Crystalline D. Amorphous
469) ————— is the French word for a small shop with unusual clothing. (Answer = B)
A. Brand B. Boutique
C. Prêt a porter D. none
470) A fashion that lasts for longer time is —————- (Answer = C)
A. Fad B. Trend
C. Classic D. Interrupted fashion
471) —————are often used at the neck of a dress, or at the waist as a belt, serve as a fastener. (Answer = A)
A. bows B. button loops
C. draw string D. frog fastening
472) ——————- is the information given to the public regarding, product, policies, personnel, activities or services. (Answer = A)
A. Publicity B. Editor
C. Report D. Hangtag
473) The price paid by the retailer to the manufacturer for a garment is known as ————- (Answer = A)
A. Cost price B. Market price
C. Selling price D. Discount price
474) An attractive feature used in design is —————- (Answer = A)
A. fringing B. Darts
C. Pleat D. Vent
475) A ——————–this means made-to-measure. (Answer = C)
A. prêt-a-porter B. Ready to wear
C. Bespoke D. Fitting
476) ———————-type or garment is usually worn, while riding a horse. (Answer = D)
A. blazer B. fitted pant
C. bell bottom pant D. breeches
477) ——————– is used to remove fullness from certain parts or the garment. C
A. Gather B. Pleat
C. Dart D. Tuck
478) LEVI’S brand is the example of……(Answer = C)
A. swim wear B. Bridal
C. Jeans D. Children
479) Cotton is affected by—————— (Answer = B)
A. Alkalies B. Strong acids
C. Cold dilute acids D. All above
480) —————- is the “King of fibres”. (Answer = A)
A. Cotton B. Jute
C. Silk D. Nylon
481) Linen is the other name given to—————— (Answer = B)
A. Cotton B. Flax
C. Ramie D. Kapok
482) The short fibres are termed as—————– (Answer = B)
A. Line B. Tow
C. Filament D. Lint
483) Hacking is the term given to———–operation. (Answer = C)
A. Carding B. Scutching
C. Combing D. Pulling
484) —————— fibre which is mainly used for padding and stuffing particularly upholstery. (Answer = B)
A. Cotton B. Kapok
C. Hemp D. Urena
485) The finest quality wool is obtained from ————— (Answer = B)
A. Delaine B. merino
C. Rambouillet D. lincoln
486) The fibre obtained from Angora goat is—————-(Answer = B)
A. Alpaca B. Mohair
C. Cashmere D. Angora
487) The gummy substance which coats the silk fibre is —————— (Answer = C)
A. pectin B. glutin
C. Sericin D. None
488) In silk, the process to where twist is inserted is termed as—————- (Answer = B)
A. Reeling B. throwing
C. Spinning D. Degumming
489) The resiliency of silk is—————- (Answer = C)
A. Very good B. Good
C. Moderate D. Poor
490) The bleach which tends to destroy silk is—————— (Answer = A)
A. Chlorine B. Hydrogen per oxide
C. All of above D. None
491) The French term for ready-to-wear is———– (Answer = B)
A. Boutique B. Prêt-a-porter
C. Couturier D. haute couture
492) Couture clothing literally means ——————in French. (Answer = D)
A. Designer clothing B. Private labels
C. Mass production D. Fine sewing
493) ————is the inter face between an organization and its customers. (Answer = B)
A. Customer’s satisfaction B. Marketing
C. Fashion forecast D. Product assortment
494) Cutting V-shaped sections from the seam allowance is called —————– (Answer = B)
A. Grading B. Notching
C. Hemming D. None
495) Making straight cuts into the seam allowance is called————– (Answer = A)
A. Clipping B. Grading
C. Notching D. Hemming
496) ——————–means the Armhole; opening for a sleeve. (Answer = C)
A. Hem B. Gather
C. Armscye D. None
497) Stitches made by hand or machine to hold fabric pieces together temporarily is called————- (Answer = C)
A. Bias B. Clipping
C. Baste D. Sewing
498) Two distinct fabrics glued together as one called————- (Answer = D)
A. Canvas B. Hair Canvas
C. Heavy Fabric D. Bonded fabric
499) Inter looped stitch in also known as————– (Answer = A)
A. Chain Stitch B. Lock stitch
C. Over Lock stitch D. French seam
500) The Portion of garment above the waist is called————– (Answer = B)
A. Skirt B. Bodice
C. Sleeve D. Collar
501) Staple fibers are measured in _________ (Answer = B)
A. Yards B. Inches
C. Kilograms D. None of these
502) Cotton can also be ___________ to give the fiber added strength and luster (Answer = C)
A. Finished B. Bleached
C. Mercerized D. Calendered
503) _________ is an universal bleaching agent (Answer =B)
A. Bleaching powder B. Hydrogen peroxide
C. Copper Sulphate D. Hydrogen Chloride
504) Acid dyes are mainly applied on (Answer = B)
A. Cotton B. Wool
C. Linen D. Jute
505) Fabric is treated with heat and pressure to add luster (Answer = A)
A. Lustering B. Felting
C. Beetling D. Glazing
506) The ability of fiber to stretch and return to shape is (Answer = A)
A. Elasticity B. Crimp
C. Stretch D. Pliablity
507) ________ is one of the primary motions of the loom (Answer = C)
A. Take up B. Let-off
C. Shedding D. Denting
508) The ability of fabric to absorb moisture from body is (Answer = B)
A. Wicking B. Absorbency
C. Resiliency D. None of these
509) Squeegee is used in _________ printing (Answer = A)
A. Screen B. Roller
C. Batik D. Stencil
510) The designer of Haute Couture show a new collection _________ a year (Answer = B)
A. Once B. Twice
C. Resiliency D. Dimensional stability
511) ________ is used to stiff the fabric. (Answer =B)
A. Cleaning B. Sizing
C. Dyeing D. Printing
512) __________ is a pre-treatment for printing of cotton. (Answer = A)
A. Scouring B. Fixing
C. Calendering D. Sanforizing
513) Draw frame is a _________ machinery. (Answer =C)
A. Weaving B. Padding
C. Spinning D. Knitting
514) The process of removal of starch from the fabric is (Answer = B)
A. Sizing B. Desizing
C. Singeing D. Carbonizing
515) Yarns are marketed (bought and sold) by ____________ . (Answer =A)
A. Weight B. Diameter
C. Thickness D. Softness
516) Color fastness means that the color in the fabric is _______________ . (Answer = B)
A. Fixed B. Permanent
C. Fast D. Less
517) Clothing is a collective term for ______________, items worn on the body. (Answer = C)
A. Clothes B. Wearing
C. Garments D. Dresses
518) Texturizing is the processes that introduce. (Answer = D)
A. Coils B. Crimps
C. Zigzag shaping D. All of above
519) The Z twist is also called ________ . (Answer = C)
A. Left twist B. S twist
C. Right twist D. None of these
520) The botanical name of cotton plant is (Answer = D)
A. Oriza Setiva B. Maymosopudica
C. Asephetoda D. Gossypium
521) Indigo belongs to ________ class of dyes. (Answer = C)
A. Sulphur B. Basic
C. Vat D. Reactive
522) Who makes an addition to the word embellish. (Answer = C)
A. Jeff seid B. Robert Hook
C. Collins Thesaurus D. Thomas Edison
523) Profilm method is one of the method used to develop _________ for printing. (Answer = B)
A. Blocks B. Screens
C. Fabric D. Pigments
524) Lacemaking was a _________ art. (Answer = B)
A. Creative B. Domestic
C. Industrial D. Decorative
525) Rayon is made of (Answer = A)
A. Cellulose B. Oxygen
C. Flax D. Coal
526) Balochi embroidery alone has ________ different basic designs. (Answer = B)
A. 119 B. 118
C. 117 D. 116
527) Crewel embroidery is done with loosely twisted ________ yarn. (Answer =A)
A. Wool B. Cotton
C. Silk D. Nylon
528) Mercerization of cotton is carried out for improvement of (Answer = A)
A A. Strength and luster B. Whiteness
C. Wetting D. Stretching
529) A synonym of trouser (Answer = B)
B A. Skirt B. Pant
C. Shirt D. Gloves
530) ___________ are hard to handle as you cut and stitch. (Answer = C)
A. Loosely woven fabrics B. Sheer fabrics
C. Slippery fabrics D. Piles fabrics
531) The process of making yarn from fiber is called. (Answer = D)
D A. Knitting B. Yarning
C. Weaving D. Spinning
532) Hoodies come under which wear (Answer = B)
A. Party wear B. Casual wear
C. Swim wear D. Formal wear
533) The method of looping yarns together is called. (Answer = A)
A. Knitting B. Weaving
C. Quilting D. Stretching
534) The yarns that runs crosswise in a woven fabric is (Answer = B)
A. Warp yarns B. Weft yarns
C. Fly yarns D. Spun yarns
535) The de sizing process mainly removes (Answer =C)
A. Wax and tallow B. Dirt and color
C. Starch D. Natural impurities
536) Removal of free fiber ends from fabric by burning method is ______. (Answer = A)
A. Singeing B. Calendering
C. Embossing D. Mercerizing
537) Anti-shrink finish is given by (Answer = C)
A. Embossing B. Winch
C. Sanforizing D. Drapping
538) ___________ is known as artificial silk. (Answer = A)
A. Rayon B. Acrylic
C. Acetate D. Nylon
539) Mercerization of cotton fibers results in (Answer = A)
A. Improved strength B. Increase affinity
C. Increased bending rigidity D. Improved luster
540) ___________ is the dress fitted through the bodice, waist, and hips, and flaring out from the knees. (Answer = B)
A. Empire B. Mermaid
C. Ball gown D. A-Line
541) The size categories determined by height and body proportions. (Answer = B)
A. Measurements B. Figure type
C. Pattern size D. Selecting fabric
542) Gum Arabic is used as a _________ in the printing paste. (Answer = B)
A. Wetting agent B. Thickener
C. Softner D. Catalyst
543) For fabric sampling, the sample should not be taken from within _______ of the selvedge. (Answer = C)
A. 30mm B. 40mm
C. 50mm D. 60mm
544) Calico, a generic name for _________ products. (Answer = A)
A. Cotton B. Flax
C. Wool D. Polyester
545) The basic building block of textile is _________. (Answer = A)
A. Fiber B. Yarn
C. Thread D. Cloth
546) The lower the number_________ the needle. (Answer = A)
A. Finer B. Heavier
C. Sharper D. Stronger
547) A sharp needle is used for _________ fabrics. (Answer = C)
A. Knitted B. Textured
C. Woven D. Non-woven
548) Silk, the natural form of fiber is obtained from (Answer = B)
A. Sheep B. Cocoon
C. Jute plant D. Cotton balls
549) Fiber used for making gunny bag is (Answer = B)
A. Wool B. Jute
C. Silk D. Cotton
550) The main constituent of cotton fabric is (Answer = A)
A. Cellulose B. Fibroin
C. Aminoacids D. Lignin
551) __________ fibers are added to fabrics for decoration. (Answer = C)
A. Decorative B. Glass
C. Metallic D. Silk
552) Cotton is a _________ fiber. (Answer = A)
A. Seed B. Stem
C. Protein D. Crimped
553) The most basic of the stitching crafts, is the art of using stitches to join pieces of fabric together is called (Answer = A)
A. Sewing B. Embroidery
C. Applique D. Quilting
554) Crosswise yarns of a woven fabric is called (Answer = C)
A. Weaving B. Courses
C. Filling D. Blending
555) Which type of printing uses wood blocks? (Answer = B)
A. Roller printing B. Block printing
C. Resist printing D. Discharge printing
556) What is the source of linen? (Answer = C)
A. Cotton B. Silk
C. Flax D. None
557) Which type of printing involves a wax or other substance is printed onto a fabric. (Answer = B)
A. Block printing B. Resist printing
C. Roller printing D. Screen printing
558) The application of color to the whole body of a textile material with some degree of fastness (Answer = B)
A. Printing B. Dyeing
C. Painting D. Tie-dyeing
559) Transferring color to the surface of a fabric is called (Answer = A)
A. Printing B. Dyeing
C. Coloring D. Shading
560) Fabric passes between two heated rollers that smooth the fabric and improve the luster. (Answer = A)
A. Calendaring B. Moireing
C. Singeing D. Glazing
561) Any special treatments that are added to fabrics is called (Answer = C)
A. Sizing B. Calendaring
C. Finishing D. Bleaching
562) Which fiber has a natural tendency to felt? (Answer = A)
A. Wool B. Flax
C. Silk D. Polyester
563) What do we need to cover our body? (Answer = B)
A. Hat B. Clothes
C. Socks D. Gloves
564) The term applied to men’s, women’s and children’s wear (Answer = A)
A. Apparel B. Fashion
C. Accessories D. Brand
565) The high fashion, industry was established in _________. (Answer = C)
A. England B. Paris
C. France D. America
566) __________ is more than just clothing. (Answer = D)
A. Apparel B. Garment
C. Clothing D. Fashion
567) SDC stands for (Answer = B)
A. Sample data collection B. Society of dyers and colorists
C. System decision papers D. System of dyes and colors
568) _________ made color subcommittee. (Answer = A)
A. ISO B. SDC A
C. ASTM D. AATCC
569) Uneven warp or weft yarn defects occur in ________. (Answer = A)
A. Spinning B. Dyeing
C. Printing D. Bleaching
570) Crosswise yarns of a woven fabric is called (Answer = C)
A. Weaving B. Courses
C. Filling D. Blending
571) The increase in length that has occurred when the fabrics breaks is called (Answer = C)
A. Breaking strength B. Bursting strength
C. Breaking elongation D. Extension
572) Which fabrics often will crock more easily? (Answer = C)
A. Dyed fabrics B. Bleached fabrics
C. Printed fabrics D. Colored fabrics
573) _________ fabrics are made by interlocking the fibers with heat and moisture or with an adhesive
substance. (Answer = B)
A. woven B. Non-woven
C. Felted D. Quilted
574) = Which device is used for colorfastness to crocking? (Answer = B)
A. Fade-Ometer B. Crockmeter
C. Launder-Ometer D. Weather-Ometer
575) _________ lace has the design spread over the width of the fabric and repeated in its length. (Answer = A)
A. All over B. Mirror
C. Symmetrical D. Boader
576) Ajrak is a unique form of _________ printing. (Answer = A)
A. Block B. Screen
C. Batik D. Transfer
577) Ajraks have become a symbol of ________ culture and traditions. (Answer = B)
A. Balochi B. Sindhi
C. Punjab D. Kailash
578) Which emperors were passionate about painting, jewelry, textile architecture, poetry etc? (Answer = B)
A. Roman B. Mughal
C. Ottoman D. Japanese
579) Ajraks are usually about ________ meters long. (Answer =A)
A. 2.5 to 3 B. 1.5 to 3
C. 2.5 to 3.5 D. 2 to 3
580) Strands are plaited together by crisscrossing them diagonally and lengthwise
B A. Netting B. Braiding
C. Lacing D. Knotting
581) An open-mesh form of fabric construction that is held together by knots. (Answer = B)
A. Lacing B. Netting
C. Braiding D. Crocheting
582) Colors combined with white (Answer = A)
A. Tints B. Shades
C. Hue D. Spectrum
583) The most expensive jamawar is woven in ________. (Answer =C)
A. Punjab B. Sindh
C. Kashmir D. Baluchistan
584) The art of jewelry-making flourished in ________ century. (Answer = C)
A. 14th B. 15th
C. 16th D. 17th
585) In the late 1700s, ________ were used to spread fashion news. (Answer = C)
A. Newspaper B. Magazines
C. Fashion babies D. Media
586) __________ is the dress fitted through the bodice, waist, and hips, and flaring out from the knees. (Answer = B)
A. Empire B. Mermaid
C. Ball gown D. A-line
587) A fashion that is made to order to fit an individual client’s measurement is known as (Answer = B)
A. Pret-a-porter B. Couture
C. Mass-de-couture D. High fashion
588) ________ dye is called as ice colors (Answer = A)
A. Azoic B. Vat
C. Sulphur D. Acid
589) The staple length of cotton fiber will be in the range of ________. (Answer = B)
A. 15 to 20 B. 0.4 to 2.5
C. 7 to 12 D. 4 to 6
590) Pictures are manipulated to appear as moving images is called (Answer = A)
A. Animation B. Movies
C. Photographs D. Designing
591) The treatment that follows printing are termed…..(Answer = B)
A. Successor process B. After treatment
C. Discharging D. Crimping
592) For what work Photoshop is used? (Answer = A)
A. Graphics B. Animations
C. Programming D. Typing
593) Photoshop launched by which company (Answer = A)
A. Adobe B. Aldus
C. Eula D. Microsoft
594) The function of doctor blade in roller printing is to (Answer = B)
A. Give pressure to the roller B. Scrap off excess color paste from roller
C. Give pressure to the cloth D. Steaming the roller
595) The secondary property of a textile fiber is (Answer = B)
A. Tenacity B. Luster
C. Flexibility D. Uniformity
596) The outline, or silhouette, of an object is called (Answer = A)
A. Shape B. Space
C. Texture D. Silhouette
597) What does torso mean? (Answer = A)
A. Body B. Head
C. Limbs D. All of these
598) Fashion illustration actually corresponds the fashion design with the help of ___________. (Answer = A)
A. Drawings B. Paintings
C. Distributing D. Creating
599) The dye molecules in the dye bath move towards the fiber is called. (Answer = B)
A. Adsorption B. Absorption
C. Penetration D. Fixation
600) __________ is the raising and lowering of the warp yarn by means of a harness frame into two layers. (Answer = A)
A. Shedding B. Beating
C. Picking D. Harness frame
601) An example for a natural protein fiber is (Answer = C)
A. Cotton B. Nylon
C. Silk D. Linen
602) Which yarns are the strongest yarns and they form the base of fabric. (Answer = A)
A. Warp yarns B. Weft yarns
C. Wales D. Filling yarns
603) Applying wax to the surface of a fabric is a method of (Answer = C)
A. Tie-dye B. Shibori dyeing
C. Resist dyeing D. Fabric painting
604) The interlocking of fibers called (Answer = B)
A. Knitting B. Felting
C. Weaving D. Crocheting
605) Which fiber is sustainable (Answer = B)
A. Nylon B. Cotton
C. Polyester D. Acrylic
606) An example for a bast fiber is (Answer = B)
A. Cotton B. Linen
C. Wool D. Silk
607) Fibers that form the fleece of a sheep are (Answer = A)
A. Wool B. Cotton
C. Leather D. Nylon
608) What finish adds color to fabrics (Answer = D)
A. Quilting B. Beading
C. Brushing D. Dyeing
609) Needle sizes range from _____ to _____. (Answer = C)
A. 9 to 19 B. 8 to 16
C. 9 to 18 D. 8 to 19
610) _________ created from fibers twisted together or laid side by side is called (Answer = B)
A. Fibers B. Yarns
C. Fabric D. Texture
611) The property of bending without breaking is (Answer = B)
A. Bending strength B. Flexibility B
C. Spinning quality D. Tenacity
612) Who designs fabric weaves and prints for clothes and furnishings (Answer = C)
A. Tailor B. Pattern maker
C. Textile designer D. Stylist
613) The portion of the garment above the waist (Answer = A)
A. Bodice B. Yoke
C. Lapel D. Placket
614) The formation of small balls of fibers on the surface of fabric is called (Answer = A)
A. Pilling B. Rubbing
C. Crocking D. Napping
615) What is used for fashion forecasting (Answer = C)
A. Fashion shows B. Consumer research
C. Sales record D. All of these
616) The technique of sewing small shapes of fabric together to form larger shapes (Answer = B)
A. Quill work B. Patch work
C. Applique D. Quilting
617) What does dress designing involves (Answer = D)
A. Requirement of individual types B. Selection of materials
C. Study of the structural lines of the human figure D. All of these
618) The basic colors of red, yellow and blue (Answer = B)
A. Intermediate colors B. Primary colors
C. Secondary colors D. Complementary colors
619) A permanent finish is (Answer = A)
A. Mercerizing B. Calendaring
C. Filling with starch D. Embossing
620) A natural polyamide fiber is (Answer = D)
A. Cotton B. Jute
C. Hemp D. Wool
621) The highest rate of production in printing is obtained on (Answer = D)
A. Flatbed printing B. Block printing
C. Digital printing D. Rotary Screen Printing
622) ISO stands for (Answer = A)
A. International standard organization B. Internal standard organization
C. International society organization D. Internal system organization
623) Which yarn create wide variety of interesting textures (Answer = D)
A. Cable B. Ply
C. Monofilament D. Novelty
624) Silk, the natural form of fiber is obtained from (Answer = B)
A. Sheep B. Cocoon
C. Jute plants D. Cotton balls
625) The ability of the fiber to take up dye or color (Answer = B)
A. Absorbency B. Dye ability
C. Resiliency D. Dimensional stability
626) Who has given the new dimension to fashion illustration (Answer = A)
A. Paul Poiret B. Carl Erickson
C. Paul Iribe D. Antonio Lopez
627) The first fashion designer was (Answer = C)
A. Robertson B. Shakespeare
C. Charles Frederick Worth D. Ellie Saab
628) The typical size for a graphic design is measured in (Answer = B)
A. Pica B. Pixels
C. Points D. Inches
629) Images that are generated by computer is called (Answer = B)
A. Animations B. Graphics
C. Design D. Prints
630) ________ is a non-woven fabric where the fibers are held together by an adhesive rather than woven or knitted (Answer = B)
A. Composite fabric B. Bonded fabric
C. Blends D. None of these
631) Which device carries the weft thread that is wound on a bobbin (Answer = B)
A. Cloth beam B. Shuttle
C. Reed D. Heddle
632) Focal point or center of interest of a garment is called (Answer = C)
A. Proportion B. Silhouette
C. Emphasis D. Rhythm
633) Dyeing at fabric stage is known as (Answer = D)
A. Solution dyeing B. Top dyeing
C. Stock dyeing D. Piece dyeing
634) Under microscope, a cotton fiber looks like (Answer = B)
A. Flattened plates B. Twisted ribbon
C. Serration D. Bamboo pole
635) _________ vary in count, strength and twist (Answer = B)
A. Fibers B. Yarns
C. Fabric D. Filaments
636) The filling yarns pass over and under each warp yarn is called (Answer = B)
A. Weave B. Plain weave
C. Twill weave D. Satin weave
637) Matty Fabric has (Answer = B)
A. Huck a back weave B. Mock leno weave
C. Bedford weave D. Honey comb
638) Ceramic fibers are made of (Answer = A)
A A. Aluminum silicate B. Sodium silicate
C. Potassium silicate D. Sodium hydroxide
639) The length of filament fibers ranges between ________ yards (Answer = C)
C A. 200-1300 B. 400-1200
C. 400-1300 D. 200-1600
640) The actual fiber protein in silk is (Answer = D)
A. sericine B. alanine
C. tyrosine D. Fiborin
641) Queen of fiber is (Answer = A)
A. silk B. cotton
C. rayon D. wool
642) The short fiber are termed as (Answer = B)
A. line B. tow
C. filament D. lint
643) The images are made of _________ (Answer = B)
A. DPI B. Pixels
C. Drawing D. Pictures
644) Levis brand is the example of (Answer = C)
A. Swim wear B. Bridal
C. Jeans D. Childern
645) The type of garment is usually wear, while riding a horse (Answer = D)
A. Blazer B. Fitted part
C. Bell bottom D. breeches
646) An attractive feature used in design (Answer = A)
A. Fringing B. Darts
C. Pleat D. Vent
647) The second property of textile fiber is (Answer = B)
A. tenacity B. luster
C. flexibility D. Uniformity
648) Fibers that are measured in centimeter or inch are (Answer = A)
A. Staple fibers B. Filament fibers
C. Short fibers D. Long fibers
649) Garment cutting and manufacturing is based on (Answer = A)
A. Measurements B. Fit
C. Style D. Fullness
650) Any resource from which a designer obtains ideas (Answer = A)
A. Design resource B. Ethnic level
C. Research D. Evaluation of Collection
651) The choice of colors used in design plan is called a (Answer = C)
A. Color spectrum B. Color wheel
C. Color scheme D. Color mix
652) Secondary colors are created by mixing two (Answer = C)
A. Neutral colors B. Complementary colors
C. Primary colors D. Tertiary colors
653) Colors that are different in darkness and lightness are said to be (Answer =A)
A A. Contrasting B. Light in value
C. Dark in value D. Bright and intense
654) Which of the following are examples of warm colors (Answer = A)
A. Yellow, red and orange B. Yellow, red and blue
C. Yellow, green and blue D. Orange, purple and green
655) What is another word for the brightness of a color (Answer = B)
A. Value B. Intensity
C. Hue D. Complementary
656) Blue and orange are (Answer = B)
A. Primary B. Complementary
C. secondary D. None
657) The bleaching of cotton is done to remove (Answer = B)
A. Oils and waxes B. Natural coloring matter
C. Cellulose D. Lignin
658) Degumming is done on (Answer = B)
A. cotton B. silk
C. linen D. jute
659) Pre treatment for printing of cotton is known as (Answer = B)
A. Scouring B. Sanforizing
C. Fixing D. Calendaring
660) Acid dyes are mainly applied on (Answer = C)
A. Cotton B. Linen
C. Wool D. rayon
661) Desizing is a_______ Process. (Answer = B)
A. Dyeing B. Pre treatment
C. After treatment D. Printing
662) The hem falls right above the ankles (Answer = C)
A. Mini B. Floor
C. Ballerina D. Street
663) A straight, form fitting silhouette is (Answer = C)
A. Turmpet B. Mermaid
C. Sheath D. Tulip
664) __________ is the process of transforming a design in to its constituent flat pattern pieces and then drafting then out (Answer = A)
A. Pattern making B. Draping
C. Template D. Blocks
665) __________ and __________ are also indicating of the social; and marital status of women (Answer =A)
A. Dress and ornaments B. Sindoor
C. Black scarf and bangles D. Mangalsutra
666) __________ is a general term reffering to actual objects related to the human body (Answer = C)
A. Costume B. Wardrobe
C. Clothing D. Wear ability
667) __________ is more than just clothing (Answer = D)
A. Apparel B. Garment
C. Clothing D. Fashion
668) The finest quality of wool is obtained from (Answer = B)
A. Delaine B. merino
C. lincoln D. none
669) The resiliancy of silk is (Answer = C)
A. Very Good B. Good
C. Moderate D. poor
670) Selvedge provide extra __________ to the fabric (Answer = C)
A. strength B. Clean edges
C. both D. none
671) Fiber arrangement to get them parallel is known as (Answer = A)
A. carding B. combing
C. winding D. Drafting
672) Diameter of yarn will __________, strength will __________ . (Answer = A)
A. Increase, increase B. Decrease, increase
C. Increase, decrease D. None
673) Which is not converted into 1 ply yarn (Answer = A)
A. Linen B. Silk
C. Wool D. jute
674) Which fabric is used as 1 ply most of the time (Answer = B)
A. Linen B. Silk
C. Wool D. jute
675) A long piece of fabric, or a dress that is worn by Greeks (Answer = A)
A. Himation B. Toga
C. Tunic D. None
676) A crescent shaped fabric with one straight end is known as (Answer = D)
A. tunic B. Himation
C. Sari D. Toga
677) __________ was first stitching style (Answer = A)
A. Thonging B. Needling
C. Both D. none
678) Sewing machine was invented in __________ Century. (Answer = D)
A. 16th B. 17th
C. 18th D. 19th
679) Industrial revolution was begin in __________ . (Answer = B)
A. italy B. England
C. France D. Both A and B
680) Flying shuttle was invented by an English man in __________. (Answer = C)
A. 1731 B. 1732
C. 1733 D. 1734
681) Spining jenny was named on the (Answer =B)
A. owner B. Owners wife
C. Owners daughter D. None
682) __________ seprate the trash and dust particles from the cotton (Answer = B)
A. Twisting B. Gining
C. Winding D. Calandering
683) __________ is a place that houses many machines and many workers. (Answer = C)
A. workshop B. Studio
C. Factory D. None
684) The sewing pattern was made in….. (Answer = C)
A. 1788 B. 1789
C. 1790 D. 1791
685) Paper pattern was an __________ invention. (Answer = B)
A. Latin B. American
C. Spanish D. None
686) The first paper pattern was developed by (Answer = A)
A. Abenzir Butrick B. Eli Whitny C. John K D. James
687) __________ that stays for very short time. (Answer = B)
A. Fashion B. Fad
C. Culture D. None
688) Who introduced the high end fashion for the first time. (Answer = B)
A. John K B. Charles Worth
C. Britney Spares D. Louis vuitton
689) A tight band on the waist and long gown is known as ….. (Answer = B)
A. Bodice B. Corset
C. Belted dress D. None
690) Yellow color was widely obtained from (Answer = A)
A. Zafran B. Turmeric
C. Both D. None
691) Genisis means…… (Answer = A)
A. Origin B. History
C. Revival D. B and C
692) Fibers vary in __________ . (Answer = D)
A. Length B. Color
C. Strength D. All of the above
693) Fabric samples are always taken from __________ directions . (Answer = C)
A. Warp B. Weft
C. Both D. None
694) Factors that affects the sample testing. (Answer = D)
A. Test method B. Test efficiency
C. Test instruments D. All
695) __________ refers to anything that is capable of being woven or weaved. (Answer = A)
A. Textile B. Fashion
C. Both D. None of these
696) _____________ are old fashioned but well designed. (Answer = C)
A. Posters B. Led signs
C. Window displays D. None
697) The most suitable fabric for the use on outdoor furniture. (Answer = B)
A. Cotton B. Polyester fiber
C. Rayon D. Both A&B
698) Warp in different colors and weft in one color create (Answer = B)
A. Shot effect B. Stripe effect
C. Cross over effect D. Check style
699) Both warp and weft in different colors (Answer = D)
A. Shot effect B. Stripe effect
C. Cross over effect D. Check style
700) Printing is also defined as (Answer = C)
A. Dyeing B. Coloring
C. Localized dyeing D. None
701) ____________ fabric can be identified by looking at the back side of the fabric where there is no color or design on face side (Answer = A)
A. Printing B. Dyeing
C. Batik D. Shibori
702) Dyes like vat and reactive are mostly used for (Answer = A)
A. Cotton B. Wool
C. Linen D. Viscose
703) Basic approaches to printing a color on a fabric are….. (Answer = B)
A. 2 B. 3
C. 4 D. 5
704) The printing approach that imprinted the dye in the paste form to form a pattern are.. (Answer = A)
A. Direct B. Discharge
C. Reactive D. None
705) Oldest and simplest way of printing is (Answer =D)
A. Roller B. Screen
C. Rotary D. Block
706) An indirect method of printing in which dyes are transferred from paper to a thermoplastic fabric
under controlled condition is known as (Answer = C)
A. Roller B. Screen
C. Transfer D. None of these
707) There are _________ of resist printing. (Answer = B)
A. 1 B. 2
C. 3 D. 4
708) Most advanced type of printing is (Answer = A)
A. Digital B. Roller
C. Rotary D. None
709) ____________ print of varieties of flowers huge or small, bunch or single known as (Answer = C)
A. Classical B. Ethnic
C. Floral D. Traditional
710) The culture of any particular place can be described in ____________ print. (Answer = A)
A. Classical B. Ethnic
C. Floral D. Traditional
711) __________ is the final process given to a textile material for desirable feel and good appearance (Answer = B)
A. Dyeing B. Finishing
C. Printing D. Calendaring
712) ___________ finish involves a chemical change in fiber structure and do not alter through the life of the fabric (Answer = D)
A. Temporary B. Durable
C. Semi durable D. Permanent
713) ___________ finish are removed or diminished the first time the article is laundered. (Answer = A)
A. Temporary B. Durable
C. Semi durable D. Permanent
714) Finish that improves the performance properties of the fabric is known as (Answer = A)
A. Functional B. Aesthetics
C. Both D. None of these
715) Resist the penetration of water into or through the fabric (Answer = B)
A. Water repellent B. Water proof
C. Both D. None of these
716) Stiffening agents are applied to the cloth to increase (Answer = D)
A. weight B. Thickness
C. Luster D. All of the above
717) The process of screen printing involves printing _________ color . (Answer = A)
A. Each B. 1
C. 2 D. 3
718) _________ is a substance that can absorb light and reflect some lights to show color but it is water
insoluble. (Answer = B)
A. Dye B. pigment
C. Chemical D. Finish
719) Azo dyes are first produced in (Answer =C)
A. 1861 B. 1862
C. 1863 D. 1864
720) _________ is the last process of dyeing of goods. (Answer = A)
A. Garment B. Yarn
C. Fiber D. None
721) Textile auxiliaries are (Answer = D)
A. Salt B. Water
C. Soda ash D. All of the above
722) _________ is much prone to wrinkle easily. (Answer = A)
A. Cotton B. Silk
C. Chiffon D. Organza
723) Photoshop was created in _________ . (Answer = A)
A. 1988 B. 1989
C. 1990 D. 1991
724) _________ tool selects areas based on pixels of similar values. (Answer = B)
B A. Pen B. Magic wand
C. Slicing D. Cropping
725) Which of the following structures makes wool suitable for dyeing (Answer = A)
A. Amorphous structure B. Morphological structure
C. crystalline D. Hydrophobic
726) Advanced, vector-based editing software used to create logos, graphics, cartoons and fonts is called (Answer = C)
A. Photoshop light room B. Adobe Photoshop
C. Adobe illustrator D. Photoshop CC
727) ___________ creates fashion wears. (Answer = B)
A. Fashion followers B. Fashion innovators
C. Fashion role models D. Fashion victims
728) Hoodies comes under which wears. (Answer = B)
A. Swim B. Casual
C. Sports D. Formal
729) A permanent finish is (Answer = A)
A. Mercerization B. Glazing
C. Lustering D. Calendering
730) Acid dyes are mainly applied on (Answer = C)
A. Cotton B. Linen
C. Wool D. Rayon
731) _________ is an after treatment for printed cloth. (Answer = A)
A. Steaming B. Scouring
C. Sizing D. Glazing
732) _________ is resist style printing. (Answer = A)
A. Batik B. Screen
C. Roller D. Stencil
733) Squeegee is used in _________ printing. (Answer = B)
A. Batik B. Screen
C. Roller D. Stencil
734) Which design accent the persons height. (Answer = A)
A. Vertical lines B. Horizontal
C. Diagonal D. Check
735) Which shape is formed by the outer lines of clothing? (Answer = A)
A. Silhouette B. Diagonal
C. Vertical D. Horizontal
736) ________ is an element of design that can be seen or felt. (Answer = B)
A. Proportion B. Texture
C. Rhythm D. Balance
737) Denier is the term that is applied to the (Answer = B)
A. Fiber B. Yarn
C. Fabric D. None
738) In ________ dyeing is called as bandhani (Answer = C)
A. Italy B. China
C. India D. Japan
739) Japanese art of paper folding is (Answer = A)
A. Origami B. Ikebana
C. Karaoke D. Haiku
740) Pablo Picasso belonged to which city . (Answer = C)
A. China B. France
C. Spain D. Italy
741) Which animal emphasizes peace in art. (Answer = D)
D A. Cat B. Deer
C. Duck D. Dove
742) Da vinci Mona Lisa is (Answer =B)
A. Abstract B. Representational
C. Obscure D. Non representational
743) Aesthetics deals with objects that are (Answer = B)
A. Essential B. Non essential
C. Both D. None
744) Traditional art has been defines as (Answer = D)
A. Heritage B. Culture
C. Wealth D. Tradition
745) An important formal characteristics of art is (Answer = B)
A. Social meaning B. Coherence
C. Representation D. Strong emotions
746) The way to do an art critique is (Answer = D)
A. Interpret B. Describe
C. Analyze D. All
747) The principle of art that represents line and color. (Answer = A)
A. Pattern B. Unity
C. Proportion D. Emphasis
748) Which artist said ‘ everything you can imagine is real” . (Answer = B)
A. Da vinci B. Pablo Picasso
C. Vincent van gogh D. Michelangelo
749) The girl with a ________ in 17th century. (Answer = A)
A. Pearl B. Stone
C. Earing D. Scarf
750) Famous painting Mona lisa is made by…. (Answer = A)
A. Leonarda Da vinci B. Pablo Picasso
C. Vincent van gogh D. Michelangelo
751) Fashion design considered to have started in __________ century. (Answer = C)
A. 17th B. 18th
C. 19th D. None
752 __________ is a short gathered or pleated strip of fabric attached at the waistline of the dress. (Answer = B)
A. Empire B. Peplum
C. Ball gown D. A-line
753) The outline of a dress made by using accurate body measurements is called a (Answer = B)
A. Pattren B. Draft
C. Design D. Bodice
754) Hollywood of fashion world (Answer = C)
A. London B. Milan
C. Paris D. France
755) When the fashion cycle happens quite slowly, it is a __________ (Answer = B)
A. Style B. Trend
C. Fad D. Old fashion
756) The process of separating cotton fiber from seed is called ______ . (Answer = A)
A. Ginning B. Scouring
C. Roving D. Carding
757) A series of points connected together is called (Answer = B)
A. Shape B. Line
C. Space D. Illusion
758) Buttons, hooks, snaps and zippers are called (Answer = A)
A. Fasteners B. Plackets
C. Openings D. Gussets
759) The direction in which the yarn is passing in the fabric. (Answer = B)
A. Fiber B. Grain
C. Lengthwise D. Crosswise
760) Photoshop is an image _________ application. (Answer = C)
A. Sharing B. Downloading
C. Editing D. Deleting
761) Which is not the principle of design? (Answer = B)
A. Harmony B. Texture
C. Emphasis D. Balance
762) A muslin garments cut from a first pattern is called (Answer = A)
A. Sample B. Template
C. Test D. Dress
763) Denier is the term applied to the strength of (Answer = B)
A. Fiber B. Yarn
C. Fabric D. Cotton
764) A____________ is a group of individuals who live together in a particular area. (Answer = C)
A. Culture B. Values
C. Society D. Custom
765) ______________ were laced together to form the first woven fabric. (Answer = C)
A. Threads B. Fabric
C. Grasses D. Laces
766) Which of the following fibers is a synthetic fiber. (Answer = A)
A. Polyester B. rayon
C. flax D. wool
767) The simplest loom for plain weave has ___________ harnesses. (Answer = A)
A. Two B. Four
C. Three D. Six
768) The secondary property of textile fiber is (Answer = A)
A. Luster B. Tenacity
C. Flexibility D. Uniformity
769) Yarn is produced by spinning (Answer = B)
A. Fabric B. Fibers
C. Cloth D. None of these
770) In mercerization process ______ is used. (Answer = B)
A. Sulphuric Acid B. Sodium Hydroxide
C. Hrdrochloric acid D. Sodium Carbonate
771) The interloping of fibers is called (Answer = B)
A. Felting B. Knitting
C. Weaving D. Draping
772) Calico is a generic name of (Answer = A)
A. Cotton B. Flax
C. Wool D. Polyester
773) The rubbing off of colors is called (Answer = D)
A. Rubbing B. Bleeding
C. Staining D. Crocking
774) The application of color to the whole body of a textile material with some degree of fastness. (Answer = B)
A. Printing B. Dyeing
C. Painting D. Tie-dyeing
775) Herring bone is a variation of (Answer = B)
A. Basket B. Twill
C. Satin D. Plain
776) Aerospace textile is an example of _______ textiles. (Answer = A)
A. Technical B. Medical
C. Composite D. Biotechnology
777) The amount of fullness needed for movement and comfort is called. (Answer = B)
A. Design ease B. Wearing ease
C. Comfort ease D. Pattern ease
778) __________ print is a good choice to hide small sewing mistakes. (Answer = A)
A. All-over B. Boarder
C. Mirror D. Symmetrical
779) Performance based textiles are known as ________. (Answer = D)
A. Medical B. Composite
C. Biotechnical D. Technical
780) ________ is the process of transforming a clothing design into 3d form. (Answer = A)
A. Draping B. Drafting
C. Crocking D. Napping
781) __________ finishes last throughout the life of the fabric. (Answer = B)
A. Absorbent B. Permanent
C. Durable D. Temporary
782) Dyeing of acrylic is carried out by using. (Answer = B)
A. Vat B. Cationic
C. Acid D. Disperse
783) Starches or resins are added to the fabric for extra body. (Answer = A)
A. Sizing B. Glazing
C. Lustering D. Embossing
784) Sublimation transfer printing is most suitable for (Answer = B)
A. Cotton B. Polyester
C. Silk D. Acrylic
785) Why is starch used in warp yarns? (Answer = B)
A. To increase the luster of the yarn B. To increase the strength of the yarn
C. For smoothing the yarn D. For increasing the weight of the yarn
786) Fibers mat together by the application of heat, steam and pressure is called. (Answer = A)
A. Felting B. Melting
C. Heating D. Matting
787) Fire Retardant finish is used to resist ________. (Answer = B)
A. Heat B. Fire
C. Moisture D. None
788) Scouring is the special method used for cleaning. (Answer = A)
A. Wool B. Nylon
C. Silk D. Rayon
789. How many types are the collars of shirts? (Answer = B)
A. 2 types B. 3 types
C. 4 types D. 5 types
790) The length of wool varies between ________ inches. (Answer = A)
A. 1.5 to 12 B. 2.5 to 13
C. 0.5 to 12 D. 1.5 to 13
791) Vintage fashion is also known as ____________. (Answer = B)
A. antique B. retrospective
C. classic D. old
792) Rayon, nylon and polyester are examples of (Answer = D)
A. Plant fibers B. Animal fibers
C. Natural fibers D. Synthetic fibers
793) How much threads for making a men’s shirt? (Answer = A)
A. 110 yards B. 210 yards
C. 315 yards D. 425 yards
794) Which yarns undergo less strain in the weaving process. (Answer = B)
A. Warp B. Filling
C. Courses D. Both A and B
795) Anything that wear, cover and adorns the body is called. (Answer = C)
A. Textile B. Designing
C. Clothing D. Layering
796) Different fibers combined into one yarn is called. (Answer = C)
A. Composite B. Bonded
C. Blends D. None of these
797) ______________ is the first element noticed and have huge impact on garments. (Answer = B)
A. Design B. Color
C. Theme D. Cutline
798) Focal point or center of interest of a garment is called. (Answer = C)
A. Proportion B. Silhouette
C. Emphasis D. Rhythm
799) Dyeing at fiber stage is known as (Answer = C)
A. Solution dyeing B. Top dyeing
C. Stock dyeing D. Piece dyeing
800) Currently fashion industry relies on _____________ sales. (Answer = B)
A. Ready to wear B. Mass-market
C. Haute couture D. Experimental
801) Twisting two strands of fibers together to form _________ yarn. (Answer = A)
A. Single yarn B. Double yarn
C. Ply yarn D. Cable yarn
802) Brand is an example of: (Answer = B)
A. Clothing tie-symbol B. Clothing symbols
C. Clothing signs D. Clothing tie-signs
803) The edge of a woven fabric is called. (Answer = C)
A. Felting B. Cross stitch
C. Selvage D. Edging
804) A twill weave is recognized by ________ ridges on the fabric surface. (Answer = D)
A. Horizontal B. Vertical
C. Straight D. Diagonal
805) The interlacing of two sets of yarns at right angle to each other is (Answer = A)
A. Weaving B. Knitting
C. Braiding D. Netting
806) Anything that is currently ‘in’ (Answer = B)
A. Style B. Fashion
C. Trend D. Fad
807) A fashion that is very popular for a short time. (Answer = A)
A. Fad B. Old fashion
C. Trend D. Classic
808) The surface characteristics, or feel, of an object (Answer = C)
A. Silhouette B. Shape
C. Texture D. Design
809) Changing a garment to better meet your needs (Answer = B)
A. Recycling B. Redesigning
C. Decorating D. Designing
810) The term refers to how well the fabric takes in moisture (Answer = D)
A. Durability B. Resiliency
C. Wicking D. Absorbency
811) A worn spot that develops when the fabric rubs against something. (Answer = B)
A. Resiliency B. Abrasion
C. Absorbency D. Durability
812) The first manmade fiber is (Answer = A)
A. Rayon B. Acetate
C. Nylon D. Polyester
813) A fibrous substance found in plants (Answer = C)
A. Protein B. Fibers
C. Cellulose D. Asbestos
814) Textile word derived from texere meaning (Answer = B)
A. Fabric B. To weave
C. Fibers D. Yarn
815) The standard length of belt of shalwar is (Answer = B)
A. 6 inches B. 7 inches
C. 8 inches D. 10 inches
816) Cotton, wool, silk are examples of ____________. (Answer = C)
A. Plant Fibres B. Animal Fibres
C. Natural Fibres D. Synthetic Fibres
817) The rearing of silkworms for obtaining silk is known as (Answer = B)
A. Horticulture B. Sericulture
C. Apiculture D. Silviculture
818) Heat transfer printing is also known as (Answer = B)
A. Fire retardant B. Thermal-wax transfer
C. Heat sensitive D. Iron press
819) Which of the following is known as protein fibre? (Answer = A)
A. Wool B. Cotton
C. Jute D. Linen
820) Which one of the following is not a natural fibre? (Answer = D)
A. Wool B. Flax
C. Cotton D. Nylon
821) Other name of filling yarn is (Answer = B)
A. Warp yarn B. Weft yarn
C. Novelty yarn D. None
822) The process of arranging two sets of yarns together to produce a fabric is known as (Answer = C)
A. Knitting B. Looping
C. Weaving D. Crochet
823) Big reels on which yarn is wounded is called (Answer = A)
A. Bobbin B. Handloom
C. Moth D. Needle
824) A key tool for making cloth is (Answer = A)
A. Sewing needle B. Sewing machine
C. Loom D. Charkha
825) Mercerization is a finish for (Answer = B)
A. Wool B. Cotton
C. Silk D. Jute
826) The process of transforming design into its constituent flat pattern pieces and then drafting it out is known as (Answer = A)
A. Pattern making B. Drafting
C. Blocks D. Template
827) The strongest natural fiber is ___________. (Answer = B)
A. Cotton B. Silk
C. Linen D. Wool
828) Staple fibres are (Answer = B)
A. Long length fibres B. Short length fibres
C. Decorative fibres D. None of these
829) Tenacity is the fibres’ (Answer = B)
A. Length B. Strength
C. Width D. Pliability
830) Which natural fibre is highly lustrous (Answer = C)
A. Wool B. Cotton
C. Silk D. Flax
831) Ability of a fibre to come back to its original shape is (Answer = A)
A. Resiliency B. Absorbency
C. Tenacity D. Both a and c
832) Which one is highly resilient fibre? (Answer = D)
A. Cotton B. Rayon
C. Flax D. Polyester
833) Basic unit of textile is (Answer = C)
A. Yarn B. Fabric
C. Fibre D. All of the above
834) Warp faced satin is ________ than the weft faced sateen. (Answer = C)
A. Lustrous B. Rough
C. Stronger D. Weaker
835) The angle of standard twill weave is always (Answer = D)
A. 90° B. 75°
C. 180° D. 45°
836) A style that is popular in the present or a set of trends that has been accepted by a wide audience (Answer = C)
A. Style B. Fad
C. Fashion D. Classic
837) The process which is done for the removal of substances from grey goods is (Answer = B)
A. Scouring B. Singeing
C. Bleaching D. Mercerization
838) The process that gives a velvety surface (Answer = A)
A. Napping B. Brushing
C. Beetling D. Calendering
839) Weighting process is for (Answer = D)
A. Cotton B. Wool
C. Nylon D. Silk
840) Printing in which wooden blocks carved with a design to create a design is (Answer = C)
A. Roller printing B. Screen printing
C. Block printing D. Heat transfer printing
841) The technique which is used whenever long runs of fabric are to be printed with the same design (Answer = A)
A. Roller printing B. Screen printing
C. Block printing D. Heat transfer printing
842) Finishes that are used improve the performance properties of fabrics (Answer = C)
A. Chemical finishes B. Mechanical finishes
C. Functional finishes D. Aesthetic finishes
843) Pretreatment process involving burning of projecting fibers or filament splinters from the surface of a fabric (Answer = D)
A. Desizing B. Precuring
C. Precuring D. Singeing
844) Color is a design’s (Answer = C)
A. Principle B. Value
C. Element D. None
845) Which color cannot be made by mixing any other colors? (Answer = A)
A. Yellow B. Green
C. Grey D. Purple
846) _______ textiles are versatile fibrous fabrics designed to stay treat wounds and medical conditions. (Answer = D)
A. Composite B. Technical
C. Non woven D. Medical
847) Dullness and brightness of colors is known as (Answer = B)
A. Value B. Intensity
C. Hue D. both b and c
848) Hue is also known as (Answer = C)
A. Intensity B. Value
C. Color D. None
849) Colors that are located close together on a color wheel are known as (Answer = B)
A. Complementary colors B. Analogous colors
C. Monochromatic colors D. Tertiary colors
850) Which of the following are examples of cool colors? (Answer = B)
A. Orange, green and purple B. Blue, green and violet
C. Yellow, blue and red D. White black and brown
851) Which one of the following are obtained by adding black to a hue? (Answer = D)
A. Tints B. Neutrals
C. Secondary colors D. Shades
852) Which color is the result of mixing of yellow + blue? (Answer = D)
A. Violet B. Orange
C. Brown D. Green
853) Cutting shapes from textile fabrics and attaching them to another fabric or garment in order to decorate the base material. (Answer = A)
A. Applique B. Quilting
C. Weaving D. Gimp
854) Designs in which each side of an item of apparel is different in structure than the other side (Answer = A)
A. Asymmetrical B. Symmetrical
C. Radial D. None of the above
855) A hand technique for decorating textiles in which parts of the fabric are covered with wax. (Answer = B)
A. Silk painting B. Batik
C. Heat transfer printing D. Screen printing
856) Diagonal direction of a woven fabric (Answer = A)
A. Bias B. Bonnet
C. Bustle D. Bustier
857) A name, label, or mark assigned to a product by its manufacturer or distributor. (Answer = B)
A. Trademark B. Brand
C. Outlet D. Both a and b
858) CAD stands for (Answer = B)
A. Creative aided design B. Computer aided design
C. Computer arranged design D. None
859) V-shaped tuck that is sewn into a garment in order to shape the fabric (Answer = A)
A. Dart B. Pleats
C. Bias D. Gathers
860) A hand technique for making small pieces of fabric and trimmings by knotting from two to four or
more yarns, strings, or cords into a variety of decorative patterns (Answer = C)
A. Weaving B. Knitting
C. Macramé D. Crochet
861) A common term used to describe clothing, attire, clothes and/or garments. (Answer = A)
A. Apparel B. Ready to wear
C. Haute couture D. All of the above
862) Superfluous ornament that adds beauty or elegance (Answer = B)
A. Beading B. Embellishment
C. Braiding D. Printing
863) Designer clothes sold in standard sizes rather than made to measure. (Answer = C)
A. Apparel B. Haute couture
C. Pret-a-porter D. None
864) Most elastic fibre is (Answer = C)
A. Nylon B. Polyester
C. Spandex D. Acrylic
865) A long or short, usually sleeveless, straight, tubular garment (Answer = A)
A. Tunic B. Chiton
C. Peplos D. Himation
866) The frame which holds the heddles (Answer = A)
A. Harness B. Raddle
C. Reed D. Shuttle
867) The outside thicker edge of the cloth created while weaving . (Answer = B)
A. Draft B. Selvage
C. Shed D. Threading
868) A thin, plain weave, sheer fabric traditionally made from silk. (Answer = B)
A. Organdy B. Organza
C. Rayon D. Mohair
869) The number of warp threads per inch plus the number of weft threads. (Answer = C)
A. Weft count B. Warp count
C. Thread count D. All of the above
870) The transfer of colour from one fabric to another by rubbing. (Answer = C)
A. Barre B. Bleeding
C. Crocking D. None of these
871) A type of textile weave with a pattern of diagonal parallel ribs. (Answer = B)
A. Satin weave B. Twill weave
C. Plain weave D. Basket weave
872) Peach finish is done to improve. (Answer = A)
A. Handle and feel B. Functionality
C. Aesthetics D. None of these
873) Which of the following dyes are used for silk dyeing? (Answer = C)
A. Basic dyes B. Azoic dyes
C. Acidic dyes D. Acidic dyes
874) Dyes that do not dye the fabric directly but require a binding agent. (Answer = B)
A. Disperse dyes B. Mordant dyes
C. Direct dyes D. Vat dyes
875) Mercerization consist of (Answer = D)
A. Hydrogen per oxide B. Sulphuric acid
C. Nitrogen per oxide D. Sodium hydroxide
876) First manufactured fibre was (Answer = D)
A. Viscose B. Acrylic
C. Acetate D. Rayon
877) Which one is the most basic weave among the following? (Answer = C)
A. Basket weave B. Twill weave
C. Plain weave D. Satin weave
878) “Texere” means to (Answer = A)
A. Weave B. Stitch
C. Knit D. None
879) Linen was originated from (Answer = B)
A. Asia B. Egypt
C. Mexico D. Japan
880) Which one of the following is a direction of yarn twist? (Answer = D)
A. Z-twist B. S-Twist
C. Zero twist D. Both a and b
881) Cotton is a __________ fiber. (Answer = A)
A. Cellulosic B. Proteinic
C. Synthetic D. Man Made
882) __________ is the art of communicating fashion ideas in a visual form. (Answer = A)
A. Illustrations B. Textile Designs
C. Paintings D. Sketches
883) _____________ was considered as the earlier draper. (Answer = D)
A. Charles Dickens B. Charles James
C. Frederick Jameson Worth D. Charles Frederick Worth
884) _______________ are composed of two or more single yarns twisted together. (Answer = B)
A. Compact Yarn B. Ply Yarn
C. Cabled Yarn D. Novelty Yarn
885) Solution dyeing is mostly used for ________ fibers. (Answer = C)
A. Wool B. Natural
C. Synthetic D. Cellulosic
886) __________ are items worn on the body. (Answer = B)
A. Fabric B. Clothing
C. Textiles D. Designs
887) ___________ garments are intentionally unfinished pieces of clothing. (Answer = A)
A. Half-way B. Incomplete
C. Unstitched D. Raw
888) ______________ designers work inside the company during specific hours in a day. (Answer = A)
A. Full-time B. Freelance
C. Self employed D. In-house
889) Muslin or a grey cloth is also known as _________. (Answer = A)
A. Toile B. Kutch
C. Maison D. Finished
890) Only clothing created after ________ is considered as fashion design. (Answer = C)
A. 1856 B. 1857
C. 1858 D. 1859
891) ___________ is an article of clothing that was mass-manufactured in standard sizes. (Answer = B)
A. Haute-Couture B. Pret wear
C. Special cloths D. Costumes
892) _________ is the ability of a fabric to fall under its own weight into wavy folds of different nature. (Answer = D)
A. Texture B. Feel
C. Fall D. Drape
893) Compounds that whiten the fabric are known as _____________. (Answer = C)
A. Finishing agents B. Dying agents
C. Bleaching agents D. None of these
894) Which fiber is popularly called ‘Queen of Fibers’ (Answer = B)
A. Cotton B. Silk
C. Jute D. Flax
895) ____________ is a delicate fabric generally categories by needlelace or bobbinlace. (Answer = A)
A. Lace B. Braid
C. Handicrafts D. Macramé
896) ___________ finishing process adds stiffness to silk fabric. (Answer = B)
A. Glazing B. Weighting
C. Calendaring D. Embossing
897) The companies that provide raw materials for Fashion Pipeline are called ____________. (Answer = B)
A. Finish Product Supplier B. Component Supplier
C. Retail Distributor D. None of These
898) _______ fibers are built up of two or more different compounds, which can be of inorganic or
organic origin. (Answer = A)
A. Composite B. Bonded
C. Blends D. None of these
899) ______ rib is made with high number of picks and low number of ends. (Answer = D)
A. Selvedge B. Grain
C. Warp D. Weft
900) In a knit, the lengthwise rows of stitches are called ________________. (Answer = B)
A. Courses B. Wales
C. Warps D. None of these
901) Mercerization is just for _______ fabrics. (Answer = A)
A. Cotton B. Wool
C. Silk D. Orlon
902) Application of starch is known as ________ on fabrics. (Answer = B)
A. Finishing B. Sizing
C. Permanent D. Dyeing
903) Color is _____________ of design. (Answer = B)
A. Proportion B. Element
C. Rhythm D. All of these
904) ________ stage in fashion cycle when a strong dislike has been made for the style. (Answer = B)
A. Decline B. Obsolescence
C. Culmination D. Introduction
905) Dyes used in screen printing is in ______________ form. (Answer =D)
A. Hard B. Liquid
C. Soft D. Paste
906) In screen printing a ___________ is used to transfer ink onto a substrate. (Answer = C)
A. Net B. Plastic
C. Mesh D. Wood
907) The angle of standard twill weave is always ______. (Answer = A)
A. 45° B. 180°
C. 75° D. 90°
908) Other name for color is ______________. (Answer = D)
A. Pigment B. Dye
C. Paint D. Hue
909) Water jet loom is capable of inserting ________. (Answer = B)
A. 75rpm B. 700rpm
C. 180rpm D. 45rpm
910) The yarn count system is used for _______________ yarns. (Answer = C)
A. Complex B. Filament
C. Spun D. None of these
911) Soil release finish makes the fabric more easily wetted and less ______. (Answer = A)
A. hydrophobic B. hydrophilic
C. oleophilic D. oleophobic
912) _________ fabrics are often made from natural or recycled materials aiming to reduce the harm. (Answer = C)
A. Technical B. Natural
C. Sustainable D. None of these
913) The traditional process of fashion adoption is also called as. (Answer = C)
A. Mass Dissemination B. Trickle Up
C. Trickle Down D. Trickle Across
914) Batik is an ____ technique. (Answer = A)
A. Indonesian B. Chinese
C. Egyptian D. Asian
915) How many facets are there for a successful design. (Answer = C)
A. One B. Two
C. Three D. Four
916) ________ creates fashion. (Answer = C)
A. Victims B. Followers
C. Innovators D. Models
917) The fabric come out from the loom is known as _________. (Answer = C)
A. White goods B. Black goods
C. Grey goods D. None of these
918) ________________ gives cotton fiber, strength and luster. (Answer = A)
A. Mercerization B. Silhouette
C. Emphasis D. Bleaching
919) Thickly woven edge of the fabric is _____________. (Answer = A)
A. Selvage B. Bias
C. Dyeing D. Printing
920) Which of the following is cottage industry. (Answer = C)
A. Cement B. Textile
C. Handicraft D. Sugar
921) The biggest industry of Pakistan is _________. (Answer = B)
A. Cement B. Textile
C. Paper D. Sugar
922) Ends and picks are known as _________ and __________ respectively. (Answer = A)
A. Warp and filling B. Filling and warp
C. None of these D. Both of these
923) The hand finished edge of the garment is called _____________. (Answer = B)
A. Yoke B. Hem
C. Lepel D. Trim
924) _______________ technique is used to prevent the edge from fraying. (Answer = B)
A. Seam allowance B. Seam Finish
C. Seam D. None of these
925) _________ refers to the relative size and scale of various elements in a design. (Answer = C)
A. Rhythm B. Balance
C. Proportion D. Harmony
926) Lightness in the intensity of a color is called ______________. (Answer = C)
A. Shade B. Value
C. Tint D. None of these
927) ______________ are used create volume in a garment. (Answer = B)
A. Gathers B. Pleats
C. Darts D. Hem
928) The most commonly used fiber in carpet is __________. (Answer = A)
A. Wool B. Nylon
C. Rayon D. Cotton
929) The pleasing arrangement of all parts of garment is called ______________. (Answer = B)
A. Balance B. Harmony
C. Proportion D. Rhythm
930) Which city is famous for the textile mills that produce finest worsted suiting in the world. (Answer = D)
A. Haripur B. Lawrencepur
C. Karachi D. Faisalabad
931) When heat and moisture are applied to wool, the scales spread and soften slightly. (Answer = B)
A. Compression B. Felting
C. Calendaring D. None of these
932) The less expensive copies of designer’s garments are called __________. (Answer = A)
A. Knock-off B. Seconds
C. B-Grade D. Both a & b
933) _________ is the type of knitting. (Answer = B)
A. Macramé B. Crocheting
C. Braiding D. Embroidery
934) The protein of silk fiber is called _______. (Answer = C)
A. Sericin B. Keratin
C. Fibron D. Amino acid
935) In the weaving operations, inserting filling yarns through the shed is called _____________. (Answer = B)
A. Shedding B. Picking
C. Beating up D. Taking up
936) __________ process increases the strength of cotton as much as 20%. (Answer = D)
A. Singeing B. Calendaring
C. Bleaching D. Mercerizing
937) The word synthetic means ___________. (Answer =B)
A. Natural B. Artificial
C. Man-made D. Regeneration
938) Soft unstitched folds of fabric, used to control fullness are known as __________. (Answer = A)
A. Gathers B. Pleats
C. Notches D. Dents
939) Batik is a technique of __________. (Answer = B)
A. Dye resist dyeing B. Wax resist dyeing
C. Tie and dye D. Block resist dyeing
940) _________ is considered as most strongest fiber. (Answer = A)
A. Glass fiber B. Polyester
C. Cotton D. Wool
941) Metallic fibers are only used for (Answer = C)
A. Strength B. Apparel
C. Decoration D. None of above
942) _________ remains in fashion for a long period of time (Answer = A)
A. Classic B. Style
C. Fad D. None of these
943) Rayon is made of __________. (Answer = B)
A. Flax B. Cellulose
C. Protein D. None of these
944) In satin weave, the weft faced is known as (Answer = A)
A. Sateen B. Satin
C. Floats D. Both a & b
945) _________ fabric requires more yarn per cloth cover & ravels at the end (Answer = A)
A. Knitted B. Textile composite
C. Knit sew D. Tufted
946) Secondary motion of weaving is_______. (Answer = D)
A. Battening B. Picking
C. Shedding D. Wrap protection
947) ______ rib is made with high number of picks and low number of ends. (Answer = B)
A. Wrap B. Weft
C. Basket D. Twill
948) The most used synthetic fiber is _________. (Answer = D)
A. Acrylic B. Orlon
C. Nylon D. Polyester
949) Two layers are locked together with a chain stitch in ____ fabric. (Answer = D)
A. Stitch through B. Tufting
C. Woven D. Knit-sew
950) Warp faced satin is____ than the weft faced sateen. (Answer =D)
A. Lustrous B. Rough
C. Weaker D. Stronger
951) In which weave, cell like appearances with ridges, long floats and hollows are found? (Answer = C)
A. Devon Huck-A-Back weave B. Mock leno weave
C. Ordinary Honeycomb D. Bedford Cord
952) Which of the following is the odd one out with regards to enhancing whiteness in textile
materials? (Answer = D)
A. Bleaching B. Optical Brightner
C. Bluing agent D. Alkali
953) How many facets are there for a successful design. (Answer = C)
A. One B. Two
C. Three D. Four
954) Figured effects are more prominent in__________weave. (Answer = B)
A. Lappet B. Swivel
C. Plain D. Sateen
955) A sleeve cut wide at the armhole and tapering to the wrist is ____________. (Answer = A)
A. Dolman sleeve B. Puff sleeve
C. Plain sleeve D. Tulip sleeve
956) Water jet looms are capable of inserting ______________. (Answer = A)
A. 700 picks per minute B. 75 picks per minute
C. 180 picks per minute D. 45 picks per minute
957) ________________is a style that is popular in the present or a set of trends that has been accepted by a wide audience. (Answer = C)
A. Style B. Fad
C. Fashion D. Classic
958) In which stage of the fashion cycle do consumers reject a style and start looking out for
something new (Answer = D)
A. Decline B. Introduction
C. Peak D. Rejection
959) Dart Manipulation of the front bodice consists of __________ types. (Answer = A)
A. 13 B. 14
C. 6 D. 8
960) A primary property of a textile fiber which refers to adequate strength is (Answer = D)
A. Cohesiveness B. Flexibility
C. Density D. Tenacity
961) Find the odd one out (Answer = D)
A. Cotton B. Jute
C. Linen D. Silk
962) The basis of poly propylene fibers are (Answer = B)
A. Methane B. Propane
C. Propylene D. Ethane
963) The secondary property of a textile fiber is (Answer = B)
A. Tenacity B. Luster
C. Flexibility D. Uniformity
964) Acrylic is used to create __________. (Answer = C)
A. Fake fur B. Luggage
C. Sweaters D. All of above
965) Tenacity is the term usually applied to the strength of (Answer = A)
A. Fibre B. Yarn
C. Fabric D. Cotton
966) The process of raising and lowering of harness in a weaving loom is called (Answer = B)
A. Picking B. Shedding
C. Drawing D. Beating
967) Which of the following pairs of colours is an example of complementary colours? (Answer = B)
A. blue violet B. yellow violet
C. red orange D. blue green
968) The primary property essential for a fibre is (Answer = C)
A. Luster B. Density
C. Length to width ratio D. Resiliency
969) The ability of a fiber to return to shape following compression, bending or similar deformation is termed as (Answer = C)
A. Elastic recovery B. Elongation
C. Resiliency D. Spinning quality
970) If the arrangement of molecules within the fibre are parallel to each other and to the longtitudinal axis of the fibre then (Answer = B)
A. High orientation B. Low orientation
C. Crystalline D. Amorphous
971) An important type of associative force in textiles (Answer = C)
A. Carbon bonding B. Hydrogen bonding
C. Oxygen bonding D. Coo bonding
972) This is effectively used on many areas of a garment (Answer = C)
A. Riping B. Embroidery
C. Draq string D. Rouleau
973) This is inserted in the casing or hem to pull area or fulled together (Answer = A)
A. A cord B. Hook
C. Velcro D. Elastic
974) One strip is covered with hooks and the other with very fine loops. (Answer = B)
A. Lace B. Velcro
C. Zippers D. Buttons
975) Which of the following fabric is suitable for evening gown? (Answer = A)
A. Satin B. Flannel
C. Garbardine D. Silk tweed
976) _______ are used in a variety of ways on different areas or a garment such as the yolles, sleeves, skirt or panel lines. ? (Answer = A)
A. Gathering B. pleats
C. Darks D. Tucks
977) NIKE’ is the example of the brand name of (Answer = A)
A. Sports wear B. Men’s wear
C. Children’s wear D. None
978) The class of dyes, which are formed from to components usually, referred to as naphthols and bases. (Answer = C)
A. Dispersed dyes B. Sulphur dyes
C. Azoic dyes D. Reactive dyes
979) For the application of basic dyes on cotton this process is essential. (Answer = A)
A. Mordanting B. Acetylating
C. Coupling D. Vatting
980) The transverse group of threads running from one selvedge to the other in a cloth is termed. (Answer = A)
A. Pile B. Weft
C. Warp D. End
981) To enable the printer to make correct registration of the block on the cloth ________ are often fixed round the sides of the block. (Answer = B)
A. Leather Strips B. Pitch Pins
C. Clamps D. Brass clips
982) Sensitising solution is used in the preparation of ___________ for printing. (Answer = A)
A. Screen B. Stencil
C. Roller D. Block
983) The length of one lea of yarn is _________ yards. (Answer = B)
A. 100 B. 120
C. 36 D. 40
984) The fiber which was popularly termed as ‘Artificial silk’ is. (Answer = D)
A. Nylon B. Urena
C. Arnol D. Rayon
985) The gummy substance which coats the silk fibre is (Answer = C)
A. Pectin B. Glutin
C. Sericin D. All the above
986) In silk, the process to where twist is inserted is termed as (Answer = B)
A. Reeling B. Throwing
C. Spinning D. Degumming
987) Degumming is carried out to remove (Answer = C)
A. Pectin B. Gluten
C. Sericin D. None of the above
988) The resiliency of silk is (Answer = C)
A. Very good B. Good
C. Moderate D. Poor
989) Silk is affected by (Answer = D)
A. Alkalies B. Acids
C. Chlorine D. All the above
990) Conversion of yarn into fabric is carried out by a process termed as (Answer = B)
A. Weaving B. Spinning
C. Combing D. Carding
991) Couture clothing literally means in French (Answer = D)
A. Designer clothing B. Private labels
C. Mass production D. Fine sewing
992) _______ is the inter face between an organization and its customers. (Answer = B)
A. Customer’s satisfaction B. Marketing
C. Fashion forecast D. Product assortment
993) Garments having two legs, called (Answer = B)
A. Upper torso B. Bifurcated garments
C. Begging D. Bespoke
994) Basic pattern used to produce a basic fitted garment. (Answer = A)
A. Sloper B. Torso
C. Body size D. Making
995) Temporary stitches, also means (Answer = C)
A. Back stitch B. Overlock
C. Basting D. Feed of the arm
996) Intensity of color-brightness versus dullness (Answer = C)
A. Vibgyor B. Hue
C. Chroma D. Magenta
997) Inter looped stitch in also known as (Answer = C)
A. Lock stitch B. Over lock stitch
C. Chain stitch D. French seam
998) Heavy outer line on pattern piece is the (Answer = B)
A. Circles B. Cutting line
C. Notches D. Small arrows
999) In costing of a garment FOB stands for ___________. (Answer = A)
A. Freight on Board B. Food on Board
C. Feight on Board D. Fear on Board
1000) __________________ create fashion. (Answer = D)
A. Fashion role model B. Fashion followers
C. Fashion victims D. Fashion innovators
References:
- Apparel Manufacturing Technology By T. Karthik, P. Ganesan and D. Gopalakrishnan
- Textile Engineering – An Introduction Edited by Yasir Nawab
- Fibers to Fabrics by Bev Ashford
- Introduction to Textile fibers H. V. Sreenivasa Murthy
- https://www.textileblog.com/short-questions-and-answers-on-textile-engineering-for-interview/
- https://www.textileblog.com/terminology-of-textile-and-apparel-industry/
- https://www.textileblog.com/200-apparel-terms-and-definitions-for-professionals/
- http://uaf.edu.pk/
You may also like:
- Strategies of Effective Interviewing for Apparel Merchandising
- Job and Academic Viva Questions and Answers on Textile Fibres
- Self Development for Unemployed and Fresh Graduates in Textile Sector
- Viva Questions and Answers for Fashion Design Students and Professionals
- Interview Questions for Industrial Engineering Job in Apparel Industry
- Grading and Pattern Making: Job Interview Questions
- Interview Questions on Dress Draping and Fitting
- Interview Questions and Answers for Weaving and Knitting
- Interview Questions and Answers for Apparel Jobs
- Yarn Manufacturing Job Interview Questions and Answers
Founder & Editor of Textile Learner. He is a Textile Consultant, Blogger & Entrepreneur. Mr. Kiron is working as a textile consultant in several local and international companies. He is also a contributor of Wikipedia.






Very educative, thanks 🙏
I fell like giving exam but here the answers are written. Thank you for such a post. I have never seen a MCQ’s like this. Great initiative.
GOOD WORK GUYS.I PERSONALLY ENJOYED YOUR QUESTIONS
Thank you so much 🙏
Thank you so much