Last Updated: February 12, 2022
Textile Manufacturing Process:
Clothing is the basic human need. For hiding shame and also protecting from the inclemency of weather clothing is essential for human being. Clothing is the final product of textile manufacturing. Textile manufacturing or production is a very complex process. The range of textile manufacturing is so long. It starts from fiber to finished products. Flow chart of textile manufacturing is given below:

Process Flow Chart of Textile Manufacturing:
Spinning
↓
Weaving
↓
Dyeing +Printing+ Finishing
↓
Garments Manufacturing
This is the basic and primary flowchart of textile manufacturing. In this article I will give flow chart of all branches of textile engineering like as spinning, weaving, dyeing, printing, finishing and garment manufacturing.
Flow Chart of Spinning
Blow room
↓
Carding
↓
Drawing
↓
Combing
↓
Drawing
↓
Roving Manufacturing
↓
Ring Spinning
Flow Chart of Weaving
Yarn from spinning section
↓
Doubling and Twisting
↓
Winding
↓
Creeling
↓
Warping
↓
Sizing
↓
Winding on weaver’s beam
↓
Weaving
Flow Chart of Dyeing
Inspection of grey cloth
↓
Stitching
↓
Cropping
↓
Brushing
↓
Singeing
↓
Desizing
↓
Scouring
↓
Bleaching
↓
Souring
↓
Washing
↓
Drying
↓
Mercerizing
↓
Dyeing
↓
Aftertreatment
↓
Finishing
↓
Inspection
↓
Packing
↓
Baling
Flow Chart of Printing
Inspection of grey cloth
↓
Stitching
↓
Cropping
↓
Brushing
↓
Singeing
↓
Desizing
↓
Scouring
↓
Bleaching
↓
Souring
↓
Washing
↓
Drying
↓
Mercerizing
↓
Printing
↓
Aftertreatment
↓
Finishing
↓
Inspection
↓
Packing
↓
Baling
Flow Chart of Textile Finishing
Dewatering
↓
Slitting
↓
Stentering
↓
Compacting
↓
Final inspection
↓
Packing
↓
Bailing
↓
Deliver
Flow Chart of Garment Manufacturing
Design / Sketch
↓
↓
↓
Production Pattern
↓
↓
↓
↓
↓
Sorting/Bundling
↓
Sewing/Assembling
↓
↓
Pressing/ Finishing
↓
↓
Packing
↓
Dispatch
You can see all process shortly in this video:
https://www.youtube.com/watch?v=5nUjGNDImIk
Founder & Editor of Textile Learner. He is a Textile Consultant, Blogger & Entrepreneur. Mr. Kiron is working as a textile consultant in several local and international companies. He is also a contributor to Wikipedia.






very usefull