3XDRY® Textile Finishing Technology: Function and Benefits
Md. Mehedi Hasan Shibli
Department of Textile Engineering
Northern University Bangladesh
Email: [email protected]
Flash dried fabrics:
Schoeller Textil’s 3XDRY® textile finishing technology provides fabrics with multi-functional moisture-management properties. It is an application of technical textile. 3XDRY® finish treatment does not affect the appearance, hand or the air permeability features of the fabric.

3XDRY®: The feel-good technology
The feel-good technology 3XDRY® makes textiles water and stain repellent on the outside and water absorbent on the inside. Cloths finished with 3XDRY® keeps the body dry, minimizes perspiration marks and stimulates a cooling effect. Founded and Manufactured by schoeller technology (Switzerland).

The Function of 3XDRY® Finish:
The 3XDRY® – Advance moisture management- finish combines two technologies in one textile: on the outside textiles is finished with a water repellent function(Hydrophobic), whereas on the fabrics inside it absorbs perspiration (Hydrophilic). As a result, it reliably repels moisture from the outside. Moisture resulting from perspiration is quickly absorbed from the inner side of the textile, transported away from the body and distributed over a large area surface area. The appearance , hand or the air permeability features are not influenced by the 3XDRY®-finish.
Benefits of 3XDRY® Finishing:
1. Minimizes perspiration marks
Only the inside of the textile absorbs moisture. Perspiration marks are practically invisible from the outside.

2. Stimulates a cooling effect
With 3XDRY®, perspiration evaporates close to the body. This assists the natural cooling function of the body and ensures more energy during active phase.

3. Repels water and stains
Textiles with 3XDRY® treatment are significantly less susceptible to water, dirt and stains.

More advantages of 3XDRY® Textile Finishing Technology:
- Advanced Moisture-Management System
- Enables the skin to breathe
- Ensures wear-comfort you can see and feel
- Is applicable on all textiles (cotton, synthetics etc)
Schoeller says that 3XDRY feel good technology is increasingly being discovered for the workwear sector, now that the versatile functions have proven themselves in sports and sportswear. 3XDRY was developed in Switzerland in accordance with the criteria of the bluesign standard, a stringent textile standard for EHS criteria (Environment, Health, and Safety).
You may also like:
- Nanotechnology in Textiles: A New Field for Research and Development
- Recent Innovations in Nano-finishing in Textiles
- Value Addition Finishes for Textiles
- Antibacterial Finishes on Textile Materials
- Textile Finishing: Beautification Process of Fabric
- Self Cleaning Textiles: New Concept of Textile Finishing
- Fragrance Finishing of Textiles: Finishing Techniques and Future Scope
Founder & Editor of Textile Learner. He is a Textile Consultant, Blogger & Entrepreneur. Mr. Kiron is working as a textile consultant in several local and international companies. He is also a contributor to Wikipedia.