Name of the experiment:
Study on the production calculation of single truck single jersey circular knitting machine.
Introduction:
Production of Single Jersey Single Truck Circular Knitting Machine means the length or weight of knitted fabrics produce per shift. A single jersey circular knitting machine’s production depends on it’s no. of needle, cylinder dia, motor r.p.m. etc.
Objects:
- To know about the gearing diagram of the machine.
- To make idea about the production of this types of this machine.
Machine Specification:
- Motor RPM = 1430
- Motor Pulley Dia = 2”
- Intermediate Pulley (1) Dia = 11”
- Intermediate Pulley (2) Dia = 2.5”
- Machine Pulley Dia = 10”
- Bevel Gear Teeth = 50T
- Cylinder Wheel Teeth = 200T
- Dia of the Cylinder = 19”
- No of Feeder = 24
- Machine Gauge = 22
- Overall Efficiency = 60%
Gearing diagram of single jersey single truck circular knitting machine:

Production Calculation:
………………CPM
Theory = —————-
………………CPI
CPM = Course Per minute
CPI = Course Per Inch
CPM = Cylinder RPM x No of Feeder
Cylinder RPM = Motor RPM x (2/11) x (2.5/10) x (50/200)
= 1430 x (2/11) x (2.5/10) x (50/200)
= 16.25
CPM = 16.25*24
= 390
Suppose CPI = 28
Production = 390/28 inch/min
= (390 x 60 x 8 x 0.91)/(28 x 36) meter/shift
= 169 meter/shift
Production Calculation in Weight:
CPM = RPM x No of Feeder x (π x d x Gauge of the machine x L)
= (16.25 x 24 x 3.1416 x 19” x 22 x 3mm x 60 x 8 x 0.6) / 1000 meter/shift
= 442478
Where,
D = Dia of the cylinder = 19”
L = Loop Length = 3 mm
Π = Constant = 3.1416
Let, count of the yarn is 20’s (English Count)
=> 840 x 20 x 0.91 meter = 0.453 kg
=> 442478 = (0.453 x 442478)/(840 x 20 x 0.91) kg
= 13.11 kg
Where,
0.91 yd = 1 meter
0.453 = 1 Pound
Production of the Single Jersey Circular Knitting Machine is 13.11 Kg Per Shift
Conclusion:
Single Jersey Circular knitting machine is primary or basic machine in the knitting technology. By this practical I came to know about the procedure of calculation the production of this type of circular knitting machine. I may use this experience in my practical job life.
You may also like:
- Types of Weft Knitting Machines with Features
- Compare between Single Jersey Single Truck & Single Jersey Four Truck Circular Knitting Machine
- Features and Uses of the Raschel Warp Knitting Machine
- Tricot Warp Knitting Machine: Parts & Working Principle
- V-bed Knitting Machine: Parts, Cam Arrangement and Knitting Action
- Difference between Raschel and Tricot Warp Knitting Machine
- Knitting Elements of Tricot Warp Knitting Machine
- List of Machinery with Details Specification of Knitting Lab
Founder & Editor of Textile Learner. He is a Textile Consultant, Blogger & Entrepreneur. Mr. Kiron is working as a textile consultant in several local and international companies. He is also a contributor of Wikipedia.