Advantages of Ozone Bleaching for Denim

Ozone Fading Techniques for Denim Finishing

ozone fading on denim

Ozone Fading Process for Denim: By using this technique, the garment can be bleached. Bleaching of denim garment is done in a washing machine with …

Read more

Categories

Advertisement

Tolker
FYI Tester

Looking for quality handbags?
Visit Verano Hill

Chivention
TextileLearner

Trending Articles!

  • Multiple Choice Questions (MCQ) for Clothing and Textiles
    Multiple Choice Questions (MCQ) for Clothing and Textiles
  • List of Top Garments Buying House in Bangladesh
    List of Top Garments Buying House in Bangladesh
  • Consumption Calculation for Woven Basic Pant/Trouser
    Consumption Calculation for Woven Basic Pant/Trouser
  • Disperse Dyes: Properties, Classification, Dyeing and Printing Method
    Disperse Dyes: Properties, Classification, Dyeing and Printing Method
  • Sanforizing Finishing and Working Principle of Sanforizing Machine
    Sanforizing Finishing and Working Principle of Sanforizing Machine
  • Different Parts of a Basic Shirt | Shirt Inspection Procedure
    Different Parts of a Basic Shirt | Shirt Inspection Procedure
  • Parts, Functions and Working Process of Stenter Machine
    Parts, Functions and Working Process of Stenter Machine
  • Difference between Natural Fiber and Man Made Fiber
    Difference between Natural Fiber and Man Made Fiber

Recent Articles

  • Eyewear for WomenStylish Eyewear for Women: From Office to Evening Glam
  • Sustainable Textile ManufacturingSustainable Textile Manufacturing: Techniques and Innovations in Reducing Waste and Energy Consumption
  • types of women's beltsTypes of Women’s Belts: Uses & Fashion Tips
  • Types of Women DressesDifferent Types of Dresses for Women
  • Racing Leather Motorcycle SuitsHonda and Yamaha Racing Leather Motorcycle Suits – Speed Meets Safety
  • Augmented Reality in fashionVirtualFudge.com – Leading Augmented App Development Company for Next-Gen Digital Experiences
  • Home InsuranceHow to Make a Successful Home and Property Insurance Claim?
  • infant clothesDifferent Types of Infant Clothes
  • Fabric laser cutting machineMethods of Fabric Cutting in Garment Industry
  • Schematic representation of a textile as a barrier to UV radiation.UV Protective Fabrics for Clothing: Properties and Uses
DMCA.com Protection Status

Textile Learner is a reference guide for textiles. It helps to update textile knowledge among the students, teachers, entrepreneurs and businessmen worldwide.

Facebook twitter linedin pinterest email

Contact

  House 28, Road 12, Sector 10,
  Uttara, Dhaka 1230.

  +8801724752452

  editor@textilelearner.net,
  textilelearners@gmail.com

 

Subscribe for Free Articles!

Enter your email address to subscribe to this blog and receive notifications of new posts by email.

Join 64.3K other subscribers
© 2010 - 2025 Textile Learner | All Rights Reserved